GATONE™ PEEK grades with glass fiber reinforcements ranging from 10- 40 % are available in natural or desired colors. Custom made grades can be developed to meet specific requirements. CHARACTERISTICS: - Outstanding chemical resistance.
- Outstanding wear resistance.
- Outstanding resistance to hydrolysis.
- Excellent mechanical properties.
- Outstanding thermal properties.
- Very good dielectric strength, volume resistivity, tracking resistance.
- Very good radiation resistance.
Information provided by Gharda. Solvay Advanced Polymers completed its acquisition of this product line in May 2006. |