MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Westlake EF601 Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Westlake EF601 is a fractional melt LDPE with excellent toughness. It is suggested in heavy duty films and shipping sacks, and in industrial shrink applications. It can be used as a bubble stabilizer in LLDPE rich films.

    Application/Uses
  • Heavy duty bags
  • Heavy duty shipping sacks
  • Industrial shrink film
  • Heavy duty C&A sheeting

FDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.

All information provided by Westlake Chemical

Key Words: Excellent toughness
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.919 g/cc0.0332 lb/in³ASTM D1505
Thickness 50.8 microns2.00 mil
Melt Flow 0.25 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.25 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 250 %250 %ASTM D882
Film Elongation at Break, TD 750 %750 %ASTM D882
Coefficient of Friction 0.500.50ASTM D1894
Dart Drop 9.84 g/micron250 g/milASTM D1709
Film Tensile Strength at Break, MD 24.1 MPa3500 psiASTM D882
Film Tensile Strength at Break, TD 18.6 MPa2700 psiASTM D882
1% Secant Modulus, MD 152 MPa22000 psiASTM D882
1% Secant Modulus, TD 193 MPa28000 psiASTM D882
 
Processing PropertiesMetricEnglishComments
Melt Temperature 182 - 204 °C360 - 400 °Fwith BUR of 1.5:1 or higher
Blow-up Ratio (BUR) 2.52.5
 
Descriptive Properties
ProcessFilm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese 505 Film LDPE polymer for flexible packaging and molding
Dow DNDA-8320 NT 7 Linear Low Density Polyethylene Resin
Dow DNDA-1082 NT 7 Linear Low Density Polyethylene Resin
Dow AFFINITY™ EG 8100G Ethylene-octene copolymer
Celanese 7205 LDPE polymer for flexible packaging and tubing

PWESF066 / 84503

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.