MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Toyobo Dyneema® SK60 High Strength Polyethylene Fiber
Categories: Other Engineering Material; Composite Fibers; Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Dyneema® posses and extremely high strength and modulus, low density, high impact strength, high durability, and excellent light and chemical stability. It is used for ropes, nets, and thread (high performance ropes/cables, sail cloth, fishing net, athletic wear, protective cloth/gloves, and chemical filters) and in composites (speaker cones, riding helmets, and sports and auto composites).

Information provided by Toyobo. Dyneema is a registered trademark of Toyobo in Japan.

Key Words: Toyobo Company
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.970 g/cc0.0350 lb/in³
Water Absorption 0.00 %0.00 %
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 3500 MPa508000 psiEstimated from tenacity
Modulus of Elasticity 110 GPa16000 ksiFiber Value
Tenacity 3.53 N/tex40.0 g/denier
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 150 °C302 °FHeat Resistance

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont™ Kevlar® 149 Aramid Fiber, diam. 12 µm
DuPont™ Kevlar® 49 Aramid Fiber
DSM Dyneema® Diamond Technology Fiber
DSM Dyneema® BT10
DSM Dyneema® Max Technology

PTOYD0 / 70852

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.