MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aleris HOGAL 5558 Aluminum 5026 H14/H34
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 5000 Series Aluminum Alloy

Material Notes: HOGAL 5558 is produced according to EN AW-5026.

Information provided by Aleris.

Key Words: AlMg4.5MnSiFe; Composition per EN 573-3:2009-08
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.66 g/cc0.0961 lb/in³AA 5083
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 88
@Thickness 5.00 - 12.0 mm
88
@Thickness 0.197 - 0.472 in
Typical
 52
@Thickness 5.00 mm,
Temperature 200 °C
52
@Thickness 0.197 in,
Temperature 392 °F
Calculated
 64
@Thickness 5.00 mm,
Temperature 150 °C
64
@Thickness 0.197 in,
Temperature 302 °F
Calculated
 84
@Thickness 5.00 mm,
Temperature 100 °C
84
@Thickness 0.197 in,
Temperature 212 °F
Calculated
 87
@Thickness 5.00 mm,
Temperature 25.0 °C
87
@Thickness 0.197 in,
Temperature 77.0 °F
Tensile Strength, Ultimate >= 250 MPa>= 36300 psiGuaranteed Minimum L-T Direction
 290 MPa
@Thickness 5.00 - 12.0 mm
42100 psi
@Thickness 0.197 - 0.472 in
Typical L-T Direction
 170 MPa
@Thickness 5.00 mm,
Temperature 200 °C
24700 psi
@Thickness 0.197 in,
Temperature 392 °F
Typical L-T Direction
 211 MPa
@Thickness 5.00 mm,
Temperature 150 °C
30600 psi
@Thickness 0.197 in,
Temperature 302 °F
Typical L-T Direction
 279 MPa
@Thickness 5.00 mm,
Temperature 100 °C
40500 psi
@Thickness 0.197 in,
Temperature 212 °F
Typical L-T Direction
 292 MPa
@Thickness 5.00 mm,
Temperature 25.0 °C
42400 psi
@Thickness 0.197 in,
Temperature 77.0 °F
Typical L-T Direction
Tensile Strength, Yield >= 200 MPa>= 29000 psiGuaranteed Minimum L-T Direction; 0.2% Offset
 230 MPa
@Thickness 5.00 - 12.0 mm
33400 psi
@Thickness 0.197 - 0.472 in
Typical L-T Direction; 0.2% Offset
Elongation at Break >= 10 %>= 10 %Guaranteed Minimum L-T Direction, in 2 inches
 14 %
@Thickness 5.00 - 12.0 mm
14 %
@Thickness 0.197 - 0.472 in
Typical L-T Direction, in 2 inches
Bend Radius, Minimum  3.5 t
@Thickness 5.00 mm
3.5 t
@Thickness 0.197 in
 4.0 t
@Thickness 8.00 mm
4.0 t
@Thickness 0.315 in
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 88.3 - 94.6 %88.3 - 94.6 %as balance
Chromium, Cr <= 0.30 %<= 0.30 %
Copper, Cu 0.10 - 0.80 %0.10 - 0.80 %
Iron, Fe 0.20 - 1.0 %0.20 - 1.0 %
Magnesium, Mg 3.9 - 4.9 %3.9 - 4.9 %
Manganese, Mn 0.60 - 1.8 %0.60 - 1.8 %
Silicon, Si 0.55 - 1.4 %0.55 - 1.4 %
Titanium, Ti <= 0.20 %<= 0.20 %
Zinc, Zn <= 1.0 %<= 1.0 %
Zirconium, Zr <= 0.30 %<= 0.30 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DWA 6092/SiC/17.5p-T6 Aluminum SiC Metal-Matrix-Composite (Al MMC), Sheet
DWA 6092/SiC/25p-T6 Aluminum SiC Metal-Matrix-Composite (Al MMC), Extruded
304 Stainless Steel
Aleris HOGAL 5558 Aluminum 5026-O/H111
Aluminum 5456-H111

NALERIS91 / 159716

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.