MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

NYCOA 2366 Plasticized Copolyamide TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE; Nylon (Polyamide PA)

Material Notes: NYCOA 2366 is an extremely flexible and transparent Nylon copolymer specifically developed for extrusion applications such as high-end fishing line, and flexible tubing.

NYCOA 2366 possesses an extremely high degree of softness, flexibility, and transparency compared to standard monofilament grade nylons.

NYCOA 2366 can be easily extruded on most equipment. This product is available in heat and light stable grades.

Information provided by Nycoa, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.08 g/cc1.08 g/ccASTM D792
Water Absorption 1.7 %1.7 %24 hours; ASTM D570
Linear Mold Shrinkage 0.012 cm/cm0.012 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.014 cm/cm0.014 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6060ASTM D2240
Tensile Strength, Yield 60.0 MPa8700 psiASTM D638
Elongation at Break 700 %700 %ASTM D638
Flexural Strength 14.0 MPa2030 psiASTM D790
Flexural Modulus 0.250 GPa36.3 ksiASTM D790
Izod Impact, Notched 8.00 J/cm15.0 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 201 °C394 °FASTM D789
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %transparent; thickness not quantified

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Liquid Silicone Rubber
Overview of materials for Polyether Block Amide (PEBA)
Overview of materials for Polyester Thermoplastic Elastomer
Arkema Pebax® 3533 SP 01 Polyether Block Amide (PEBA)
Dow DMDA-8920 NT 7 High Density Polyethylene Resin

PNYCO02 / 55537

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.