MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SCG Chemicals EL-Lene™ H6240B High Density Polyethylene Blow Molding  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: Key Characteristics:
  • Good stiffness
  • Good environmental stress cracking resistance (ESCR)
  • High compressive and impact strength
  • Good appearance
  • Odorless
  • Safe for food contact
  • Good printability

Recommended Applications: Bottles for food, juice, soft drink, milk, detergent, cosmetics products, lube oil, brake fluid, chemicals

Information provided by SCG Chemicals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.962 g/cc0.962 g/ccASTM D1505
Environmental Stress Crack Resistance 60 hour
@Temperature 50.0 °C
60 hour
@Temperature 122 °F
F50, 25% Igepal; ASTM D1693
Melt Flow 0.45 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.45 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6666ASTM D2240
Tensile Strength at Break 29.0 MPa4210 psiASTM D638
Tensile Strength, Yield 36.3 MPa5260 psiASTM D638
Elongation at Break 1100 %1100 %ASTM D638
Flexural Modulus 1.37 GPa199 ksiASTM D790
Izod Impact, Notched 1.96 J/cm
@Temperature 23.0 °C
3.67 ft-lb/in
@Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 132 °C270 °FASTM D2117
Vicat Softening Point 126 °C259 °FASTM D1525
Brittleness Temperature <= -62.0 °C<= -79.6 °FASTM D746

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SCG Chemicals EL-Lene™ H6430BM High Density Polyethylene Blow Molding
Mikro-Technik Mikrolen AST UHMW-PE
SCG Chemicals EL-Lene™ H5480S High Density Polyethylene Monofilament
SCG Chemicals EL-Lene™ H5840B High Density Polyethylene Blow Molding
ExxonMobil Paxon™ AD60-007 Blow Molding Resin

PSCGC906 / 120660

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.