MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Zeon Specialty Materials ZEONOR® 750R Cyclo Olefin Polymer  (discontinued **)
Categories: Polymer; Thermoplastic; Cyclo Olefin Polymer

Material Notes: ZEONOR® is a line of thermoplastic polyolefin resin with an excellent combination of optical and electronic properties. These unique Cyclo Olefin Polymer (COP) was developed by Zeon Corporation using proprietary technology for a wide range of electronic, automotive and packaging applications.
Zeonor® can be processed for any of these applications via injection molding, blow molding or extrusion.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 g/cc0.0365 lb/in³ASTM D792
Water Absorption <= 0.010 %<= 0.010 %ASTM D570
Moisture Vapor Transmission 0.110 cc-mm/m²-24hr-atm0.279 cc-mil/100 in²-24hr-atm40°C, 90%, 50-300μm; JIS K7129
Melt Flow 27 g/10 min
@Load 2.16 kg,
Temperature 280 °C
27 g/10 min
@Load 4.76 lb,
Temperature 536 °F
JIS K 6719
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 42.0 MPa6090 psiISO 527
Elongation at Break 140 %140 %ISO 527
Tensile Modulus 2.00 GPa290 ksiISO 527
Flexural Strength 55.0 MPa7980 psiISO 178
Flexural Modulus 1.80 GPa261 ksiISO 178
Izod Impact, Notched 0.800 J/cm1.50 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmIEC250
Dielectric Constant 2.3
@Frequency 1e+6 Hz
2.3
@Frequency 1e+6 Hz
IEC250
Dielectric Strength 70.0 kV/mm1780 kV/inASTM D149
Dissipation Factor 0.00020
@Frequency 1e+6 Hz
0.00020
@Frequency 1e+6 Hz
IEC250
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.0 µm/m-°C
@Temperature 20.0 °C
38.9 µin/in-°F
@Temperature 68.0 °F
ASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 68.0 °C154 °FASTM D648
Glass Transition Temp, Tg 70.0 °C158 °FJIS K7121
Flammability, UL94 HBHB
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 92 %
@Thickness 3.00 mm
92 %
@Thickness 0.118 in
ASTM D1003

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zeon Specialty Materials ZEONOR® 1020R Cyclo Olefin Polymer
Zeon Specialty Materials ZEONOR® 1430R Cyclo Olefin Polymer
Zeon Specialty Materials ZEONOR® 1420R Cyclo Olefin Polymer
Zeon Specialty Materials ZEONOR® 1060R Cyclo Olefin Polymer
Bhansali Engineering Abstron PT-45M ABS Antistatic Extrusion Grade

PZEONB04 / 72966

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.