MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Envalior Akulon® Diablo HT-HG0 (K-X07029) (PA66+PA6)-GF50
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/Nylon 6 Blend, Glass Fiber Filled

Material Notes: 50% Glass Reinforced, Heat Stabilized

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.58 g/cc0.0571 lb/in³dry; ISO 1183
Water Absorption 4.8 %4.8 %Sim. To ISO 62
Moisture Absorption 1.70 %1.70 %Sim. To ISO 62
Linear Mold Shrinkage, Flow 0.0037 cm/cm0.0037 in/inSim. To ISO 294-4
Linear Mold Shrinkage, Transverse 0.0056 cm/cm0.0056 in/inSim. To ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 145 MPa21000 psicond; ISO 527-1/-2
 230 MPa33400 psidry; ISO 527-1/-2
Elongation at Break 2.4 %2.4 %dry; ISO 527-1/-2
 4.6 %4.6 %cond; ISO 527-1/-2
Tensile Modulus 10.0 GPa1450 ksicond; ISO 527-1/-2
 17.0 GPa2470 ksidry; ISO 527-1/-2
Charpy Impact Unnotched  8.00 J/cm²
@Temperature -30.0 °C
38.1 ft-lb/in²
@Temperature -22.0 °F
dry; ISO 179/1eU
 8.99 J/cm²
@Temperature -30.0 °C
42.8 ft-lb/in²
@Temperature -22.0 °F
cond; ISO 179/1eU
 9.49 J/cm²
@Temperature 23.0 °C
45.2 ft-lb/in²
@Temperature 73.4 °F
dry; ISO 179/1eU
 10.0 J/cm²
@Temperature 23.0 °C
47.6 ft-lb/in²
@Temperature 73.4 °F
cond; ISO 179/1eU
Charpy Impact, Notched  1.20 J/cm²
@Temperature -30.0 °C
5.71 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 1.50 J/cm²
@Temperature 23.0 °C
7.14 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 255 °C491 °Fdry; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 245 °C473 °Fdry; ISO 75-1/-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Grupo Repol Dinalon® C1S25 PA6/PA66 Blend, Unreinforced
Envalior Akulon® Diablo HT-HG0 (K-X07029) PA66+PA6-GF50, Dry, 50% Glass Filled, Heat Stabilized
Envalior Akulon® Diablo HT50-HPG5 (PA66+PA6)-GF25
DSM Akulon® S223-TP4 (Dry) Impact Modified Nylon 66 (North America)
Envalior Akulon® K240-HP PA6-I, Dry, Heat Stabilized, Impact Modified, Extrusion Blow Molding

PDSM9757 / 161378

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.