MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Evonik Compimide® 353A Bismaleimide
Categories: Polymer; Thermoset; Polyimide, TS

Material Notes: Compimide® 353A is a low-melting eutectic mixture of bismaleimide building blocks supplied as a resolidified melt, which can be used in a wide range of BMI formulations. It is designed for the use with bismaleimide toughening modifiers Compimide® TM124 or Compimide® TM123 to form tough and temperature resistant polymer networks.

Key Words: BMI
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 400 - 750 cP
@Temperature 110 °C
400 - 750 cP
@Temperature 230 °F
 
Thermal PropertiesMetricEnglishComments
Softening Point 80.0 - 90.0 °C176 - 194 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik Compimide® 1206R55 Bismaleimide
Evonik Compimide® TM124 2,2'-Bis(3-allyl-4-hydroxyphenyl)propane
Evonik Compimide® 1224L60 Bismaleimide
Evonik Compimide® TDAB 2,4-bismaleimidotoluene
Evonik Compimide® TM123 4,4'-Bis(o-propenylphenoxy)benzophenone

PEVONIK06 / 120436

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.