MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Invista Polyclear® Conserve™ 1101F PET Copolymer Packaging Resin  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: Polyclear® Conserve™ PET 1101F is a copolymer packaging resin containing 10% post consumer recycled PET. It has a nominal intrinsic viscosity of 0.83 dl/g. Packaging made from Polyclear® Conserve™ PET 1101F has excellent clarity and is noted for its dimensional stability, which prevents shrinkage and expansion of the container. Polyclear® Conserve™ PET 1101F is formulated to be used in carbonated soft drink bottles and other applications such as packaging for food and for household goods. This polymer complies with the Federal Food, Drug, and Cosmetic Act for certain food contact applications. Polyclear® Conserve™ PET 1101F offers excellent performance in maximum throughput, stretch-blow molding applications. Preforms made from Polyclear® Conserve™ PET 1101F allow maximum blowing throughputs by quickly heating in the infrared (IR) ovens. In addition, bottles made from Polyclear® Conserve™ PET 1101F are low-stick, which eases handling issues. Containers made from INVISTA PET are lightweight, have excellent clarity, and are shatterproof. With the important advantage of being totally recyclable, PET is becoming the packaging material of choice.

Carboxyl end groups: <35 meg/kg.
Diethylene glycol content: <1.8 wt%.
Acetaldehyde content: <2.0 ppm.
Fines 0.05% through 28 mesh as manufactured.
Moisture content <0.1% as manufactured.
Chip size < 2.0 g/100 chips.
Crystallinity >50%.

The Invista PET product line has been acquired by Indorama.

Key Words: Recycled with Excellent Dimensional Stability
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density >= 0.833 g/cc>= 0.0301 lb/in³Packed
Density >= 1.39 g/cc>= 0.0502 lb/in³
Viscosity Measurement 0.81 - 0.850.81 - 0.85Intrinsic viscosity; WI No. 104 test; correlated from solution viscosity by Invista
 
Thermal PropertiesMetricEnglishComments
Melting Point <= 252 °C<= 486 °F
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %clear; thickness not quantified
 
Descriptive Properties
processBlow Molding
 Injection Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eastman Eastar GN078 Copolyester, Natural
Invista 1101 PET Copolymer Packaging Resin
Goodfellow CVD Graphene Film on PET
Eastman Eastar GN125 Copolyester, Natural
Eastman Eastar GN102 Copolyester

PKO006 / 85378

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.