MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BYK Cloisite® 93A Nanoclay
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer

Material Notes: Cloisite® 93A is an additive for plastics to improve various plastic physical properties, such as reinforcement, HDT, CLTE and barrier.

Information provided by Southern Clay Products

Southern Clay Products is now a part of BYK Additives.

Key Words: Ternary ammonium salt modified natural montmorillonite polymer additive.
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.88 g/cc1.88 g/cc
Bulk Density 0.1692 g/cc0.006111 lb/in³Loose
 0.2888 g/cc0.01043 lb/in³Packed
Loss On Ignition 40 %40 %
Particle Size <= 2.0 µm<= 2.0 µm10%
 <= 6.0 µm<= 6.0 µm50%
 <= 13 µm<= 13 µm90%
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 83835% Cloisite® reinforced Nylon 6
Tensile Strength, Ultimate 101 MPa14600 psi5% Cloisite® reinforced Nylon 6
Elongation at Break 8.0 %8.0 %5% Cloisite® reinforced Nylon 6
Modulus of Elasticity 4.657 GPa675.5 ksi5% Cloisite® reinforced Nylon 6
Flexural Modulus 3.78 GPa548 ksi5% Cloisite® reinforced Nylon 6
Izod Impact, Notched 0.270 J/cm0.506 ft-lb/in5% Cloisite® reinforced Nylon 6
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 96.0 °C205 °F5% Cloisite® reinforced Nylon 6
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 2.0 %<= 2.0 %
 
Descriptive Properties
Modifier Concentration, meq/ 100g clay90
Organic Modifiermethyl, dihydrogenated tallow ammonium
X-Ray Diffraction d-Spacing (001)23.6 Angstroms

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BYK Cloisite® 10A Nanoclay
BYK Cloisite® 30B Nanoclay
BYK Cloisite® 25A Nanoclay
BYK Cloisite® Na+ Nanoclay
BYK Cloisite® 20A Nanoclay

PSCP06 / 66555

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.