MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CeramTec Sikor® E Cordierite
Categories: Ceramic; Oxide; Aluminum Oxide; Magnesium Oxide; Silicon Oxide

Material Notes: Cordierites have low coefficients of thermal expansion and excellent resistance to thermal shock. They offer a range of thermal expansion, mechanical strength, and porosity criteria. They excel as cost-effective extruded and dry-pressed forms. Sikor® E offers higher compressive strength with slightly lower thermal shock resistance than other cordierites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.20 g/cc0.0795 lb/in³DIN EN 623-2 / ASTM-C373 / ASTM-C20
Water Absorption <= 0.10 %<= 0.10 %DIN EN 623-2 / ASTM-C373
 
Mechanical PropertiesMetricEnglishComments
Tensile Modulus 70.0 GPa10200 ksiYoung's; DINV ENV 843-2 / ASTM-F417
Compressive Strength 500 MPa72500 psiASTM C-773-88 / DIN 51067T1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  1000 ohm-cm
@Temperature 500 °C
1000 ohm-cm
@Temperature 932 °F
 1.00e+12 ohm-cm
@Temperature 100 °C
1.00e+12 ohm-cm
@Temperature 212 °F
IEC 672-1
Dielectric Constant 5.0
@Frequency 1e+6 Hz
5.0
@Frequency 1e+6 Hz
IEC 672-1 / ASTM-C150
Dielectric Loss Index 0.0070
@Frequency 1e+6 Hz
0.0070
@Frequency 1e+6 Hz
IEC 672-1 / ASTM-D149,150
 
Thermal PropertiesMetricEnglishComments
CTE, linear  0.600 µm/m-°C
@Temperature 20.0 - 200 °C
0.333 µin/in-°F
@Temperature 68.0 - 392 °F
 0.800 µm/m-°C
@Temperature 20.0 - 600 °C
0.444 µin/in-°F
@Temperature 68.0 - 1110 °F
ASTM-C373
 0.900 µm/m-°C
@Temperature 20.0 - 1000 °C
0.500 µin/in-°F
@Temperature 68.0 - 1830 °F
Specific Heat Capacity 0.500 J/g-°C
@Temperature 100 - 200 °C
0.120 BTU/lb-°F
@Temperature 212 - 392 °F
DINV ENV 821-3
Thermal Conductivity 2.00 W/m-K13.9 BTU-in/hr-ft²-°FDIN EN 821-2 / ASTM-C408
 
Descriptive Properties
ColorBrown
Thermal Shock Resistance R1 (K)250Hasselman (Experimental)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CeramTec Sikor® S Cordierite
Corning ULE® 7972 Ultra Low Expansion Glass
CeramTec 447 Cordierite
China-Yixing Longly Refractories ASM-120 Cordierite-Mullite
China-Yixing Longly Refractories ASM-125 Cordierite-Mullite

CCERA928 / 107528

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.