MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Zell-Metall Engineering Plastics Zellamid 1100
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Cast

Material Notes: Zellamid® 1100 is the registered trademark for Zell-Metall’s cast nylon 6 in different qualities.

Standard quality is a heavy duty, high impact, wear and heat resistant polyamide. It offers excellent machineability and chemical resistance. Standard color is ivory. Black and blue are available upon request.

Zellamid® 1100 is ideally suited for heavy duty plastic components and offers many advantages in comparison with steel: corrosion resistance, low weight, and low wear - e.g. for crane sheaves or carriage wheels for ropeways which are produced as finished parts by spin casting.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³
Moisture Absorption at Equilibrium 2.5 - 3.0 %2.5 - 3.0 %50% RH
Water Absorption at Saturation 6.0 - 7.0 %6.0 - 7.0 %23°C
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 83 - 8583 - 85DIN 53505
Ball Indentation Hardness 163 MPa23600 psiDIN 53456
Tensile Strength at Break 88.0 - 90.0 MPa12800 - 13100 psiDIN 53455
Elongation at Break 10 - 40 %10 - 40 %DIN 53455
Tensile Modulus 3.90 GPa566 ksiDIN 53457
 0.800 GPa
@Temperature 100 °C
116 ksi
@Temperature 212 °F
DIN 53457
Charpy Impact Unnotched NBNBDIN 53453
Charpy Impact, Notched 2.50 - 3.00 J/cm²11.9 - 14.3 ft-lb/in²DIN 53453
Coefficient of Friction 0.050 - 0.100.050 - 0.10to steel, added lubrication
 0.30 - 0.350.30 - 0.35to steel, no lubrication; ISO/DTR 7147
Abrasion 8282mm³; DIN 53516
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 µm/m-°C
@Temperature 20.0 °C
44.4 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 1.67 J/g-°C0.399 BTU/lb-°F
Thermal Conductivity 0.280 W/m-K1.94 BTU-in/hr-ft²-°FDIN 52612
Melting Point 220 °C428 °F
Maximum Service Temperature, Air 100 - 120 °C212 - 248 °Flong time operation
 120 - 140 °C248 - 284 °Fmedium time operation
 160 °C320 °Fa few hours operation
Minimum Service Temperature, Air -40.0 °C-40.0 °F
Flammability, UL94 HBHB
 
Descriptive Properties
Permissible Unit Pressure25 - 30 MPa
Time yield limitup to 5s1/1000; DIN.53444

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials TIVAR™ 88-2 UHMW-PE, Premium Lubricant Filled Lining Material
Mikro-Technik Mikrolen UHMW-PE
Mitsubishi Chemical Advanced Materials TIVAR™ 88 UHMW-PE, Premium Glass Filled, Crosslinked Linings
Zell-Metall Engineering Plastics Zellamid 1100 at 50% RH
Ensinger Tecast™ 6PA Natural Unfilled Cast Nylon 6 (PA6)

PZELL12 / 72941

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.