MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

NOVA Chemicals SCLAIR® 8107 LLDPE Injection Molding Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Injection Molded

Material Notes:

Butene Copolymer

Features:

  • Excellent ESCR
  • Excellent low temperature impact

Additives:

  • Processing antioxidant

Applications:

  • Automotive
  • Food containers
  • Custom molding

United States: SCLAIR 8107 resin complies with the specifications contained in the U.S. Food and Drug Administration (FDA) regulation 21 CFR 177.1520 for olefin polymers, para. (c) 3.2a, and may thus be used in the United States as an article or component of an article intended for use in contact with food, without temperature or food-type restrictions, subject to technical suitability.

NOVA Chemicals polyethylene resins are biologically and chemically inert.

Information provided by NOVA Chemicals®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.925 g/cc0.0334 lb/in³ASTM D 792
ESCR 100% Igepal® >= 1000 hour>= 1000 hourF50, Condition A; ASTM D 1639
Melt Index of Compound 4.8 g/10 min
@Load 2.16 kg,
Temperature 190 °C
4.8 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5252ASTM D 2240
Tensile Strength, Yield 10.5 MPa1520 psiTensile pull speed 50 mm/min; ASTM D 638
Elongation at Break 850 %850 %Tensile pull speed 50 mm/min; ASTM D 638
Flexural Modulus 0.400 GPa58.0 ksiASTM D 790
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 91.0 °C196 °FASTM D 1525
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Huntsman PE1059 Film Extrusion Polyethylene
Huntsman PE5050 Extrusion Coating Polyethylene
Aclo Accucomp Polyethylene LD0109L Low Density
ExxonMobil LLDPE LL 6100.17 Linear Low Density Polyethylene Resin
ExxonMobil LLDPE LLP 8360.29 Linear Low Density Polyethylene Resin

PNOVB053 / 194661

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.