MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo Technyl® C 206 Nylon 6, EH0
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced, Flame Retardant

Material Notes: Unreinforced Plyamide PA6, standard for fast cycling, for injection molding.

Technyl C 206 has high fluidity and good mold release, favored by a high crystallization rate. It is specially suitable for the production of technical molding with fast injection cycles.

This product is available in natural.

Information provided by Rhodia; Rhodia has been acquired by Solvay.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Key Words: Polyamide 6; PA6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ISO 1183-A
Water Absorption 1.3 %1.3 %24 hours in water at 23°C; ISO 62.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 85.0 MPa12300 psiISO 527
Elongation at Break 120 %120 %ISO 527
Tensile Modulus 2.85 GPa413 ksiISO 527
Flexural Yield Strength 115 MPa16700 psiISO 178
Flexural Modulus 1.80 GPa261 ksiISO 178
Izod Impact Resistance 0.500 J/cm²2.38 ft-lb/in²ISO 180
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 93
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 93
Dielectric Constant 3.4
@Frequency 1e+6 Hz
3.4
@Frequency 1e+6 Hz
IEC 250
Dissipation Factor 0.023
@Frequency 1e+6 Hz
0.023
@Frequency 1e+6 Hz
IEC 250
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.0 µm/m-°C
@Temperature 20.0 °C
38.9 µin/in-°F
@Temperature 68.0 °F
Melting Point 222 °C432 °FISO 3146-C
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C176 °FISO 75-2
Flammability, UL94 V-2
@Thickness 1.60 mm
V-2
@Thickness 0.0630 in
ISO 1210/UL 94
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 220 - 230 °C428 - 446 °F
Middle Barrel Temperature 225 - 235 °C437 - 455 °F
Front Barrel Temperature 230 - 240 °C446 - 464 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo Technyl® C216V30 30% Glass Filled Nylon 6
Domo Technyl® C 218 V50 50% Glass Filled, Heat Stabilized Nylon 6
Domo Technyl® C216V15 15% Glass Filled Nylon 6
Domo Technyl® C 216 Nylon 6, 30% Glass Fiber, EH0
Domo Technyl® A 218 V30 Nylon 66, 30% Glass Fiber, EH0

PRHO12 / 65945

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.