MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Cast Stainless Steel HE, ACI
Categories: Metal; Ferrous Metal; Stainless Steel; Cast Stainless Steel

Material Notes: Heat resistant

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 200200
Tensile Strength, Ultimate 655 MPa95000 psi
Tensile Strength, Yield 310 MPa45000 psi
Elongation at Break 20 %20 %
Creep Strength 9.50 MPa
@Temperature 980 °C
1380 psi
@Temperature 1800 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  17.3 µm/m-°C
@Temperature 21.0 - 540 °C
9.61 µin/in-°F
@Temperature 69.8 - 1000 °F
 20.0 µm/m-°C
@Temperature 21.0 - 1090 °C
11.1 µin/in-°F
@Temperature 69.8 - 1990 °F
Thermal Conductivity  14.7 W/m-K
@Temperature 100 °C
102 BTU-in/hr-ft²-°F
@Temperature 212 °F
 21.5 W/m-K
@Temperature 540 °C
149 BTU-in/hr-ft²-°F
@Temperature 1000 °F
 31.5 W/m-K
@Temperature 1090 °C
219 BTU-in/hr-ft²-°F
@Temperature 1990 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.20 - 0.50 %0.20 - 0.50 %
Chromium, Cr 26 - 30 %26 - 30 %
Iron, Fe 53.9 - 65.8 %53.9 - 65.8 %As remainder
Manganese, Mn <= 2.0 %<= 2.0 %
Molybdenum, Mo <= 0.50 %<= 0.50 %
Nickel, Ni 8.0 - 11 %8.0 - 11 %
Phosphorus, P <= 0.040 %<= 0.040 %
Silicon, Si <= 2.0 %<= 2.0 %
Sulfur, S <= 0.040 %<= 0.040 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Cast Stainless Steel HC, ACI
Cast Stainless Steel CA15A

MQCHEA0030a / 156653

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.