MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 1307 D Polyphenylene Sulfide (PPS), Glass Fiber
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.68 g/cc1.68 g/ccASTM D 792
Additive Loading 40 %40 %Primary Additive
Linear Mold Shrinkage 0.0010 - 0.0020 cm/cm
@Thickness 3.20 mm
0.0010 - 0.0020 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 172 MPa25000 psiASTM D 638
Elongation at Break 1.5 %1.5 %ASTM D 638
Tensile Modulus 15.9 GPa2300 ksiASTM D 638
Flexural Strength 234 MPa34000 psiASTM D 790
Flexural Modulus 15.2 GPa2200 ksiASTM D 790
Izod Impact, Notched 0.801 J/cm
@Thickness 3.20 mm
1.50 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 5.34 J/cm
@Thickness 3.20 mm
10.0 ft-lb/in
@Thickness 0.126 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 1.00e+16 ohm-cm<= 1.00e+16 ohm-cmASTM D 257
Dielectric Constant 3.8
@Frequency 1e+6 Hz
3.8
@Frequency 1e+6 Hz
Dry; ASTM D 150
Dielectric Strength 13.8 kV/mm350 kV/inShort Term; In Oil; ASTM D 149
Dissipation Factor 0.0020
@Frequency 1e+6 Hz
0.0020
@Frequency 1e+6 Hz
Dry; ASTM D 150
Arc Resistance 120 sec120 secASTM D 495
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 16.2 µm/m-°C9.00 µin/in-°FE 831
CTE, linear, Transverse to Flow 46.8 µm/m-°C26.0 µin/in-°FE 831
Deflection Temperature at 1.8 MPa (264 psi) 266 °C510 °FASTM D 648
Flammability, UL94 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 307 - 329 °C585 - 625 °F
Mold Temperature 135 - 177 °C275 - 350 °F
Drying Temperature 149 °C
@Time 21600 sec
300 °F
@Time 6.00 hour
Moisture Content 0.040 %0.040 %
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 1303 D Polyphenylene Sulfide (PPS), Glass Fiber
RTP Company RTP 1302 Polyphenylene Sulfide (PPS), Glass Fiber - UL94 V-0
Oxford Polymers PPS-40GF PPS, 40% Glass Fiber Reinforced
Omnia Plastica PPS GF40 Polyphenylenesulphide
Lotte Advanced Materials Infino® XP-2140C PPS, 40% GF

PQZTA3507 / 159111

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.