MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kolon NOPLA® KE831 PEN-PET Copolyester  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); PEN-PET

Material Notes: NOPLA® is an advanced PEN-PET copolyester which can be used for bottle, sheet & injection molding applications

UV protection & prolonged outdoor durability, enhanced gas barrier, outstanding impact strength, excellent chemical and hydrolytic resistance, higher thermal performance, excellent clarity, recyclable & non-toxic, low flammability

Information provided by US distributor, API-Kolon.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.33 g/cc0.0480 lb/in³DIN 53479; ASTM D792
Water Absorption 0.070 %0.070 %DIN 53475; ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm0.0040 - 0.0060 in/inASTM D955
Melt Flow 15 g/10 min
@Temperature 275 °C
15 g/10 min
@Temperature 527 °F
DSC
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 8888DIN 53505; ASTM D785
Tensile Strength, Ultimate 60.0 MPa8700 psiDIN 53455; ASTM D638
Elongation at Break 460 %460 %DIN 53455; ASTM D638
Flexural Yield Strength 92.2 MPa13400 psiDIN 53455; ASTM D790
Flexural Modulus 2.85 GPa414 ksiDIN 53452; ASTM D790
Izod Impact, Notched 0.539 J/cm1.01 ft-lb/inDIN 53453; ASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 60 µm/m-°C
@Temperature 20.0 °C
33 µin/in-°F
@Temperature 68.0 °F
DIN 53752; ASTM D696
Melting Point 234 °C453 °FDIN 53736; ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 77.0 °C171 °FASTM D648
Glass Transition Temp, Tg 84.0 °C183 °FDSC
Flammability, UL94 V-2V-2
 
Optical PropertiesMetricEnglishComments
Haze 1.0 %1.0 %ASTM D1003

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kolon NOPLA® KE131 PEN-PET Copolyester
DuBois Pen Kase 8 Carburizer
Kolon NOPLA® KE931 PEN-PET Copolyester
Mitsui APEL™ APL6015T Cyclo Olefin Copolymer (COC)
Kolon NOPLA® KE531HC PEN-PET Copolyester

PKOL095 / 49001

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.