MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Hexcel® HexPly® F515 Epoxy Resin, TSR9120 Carbon Tape
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes: Fiber: Toray® T700S

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 2482 MPa
@Temperature 23.0 °C
360000 psi
@Temperature 73.4 °F
Tensile Modulus 129 GPa
@Temperature 23.0 °C
18700 ksi
@Temperature 73.4 °F
Flexural Yield Strength 1234 MPa
@Temperature 23.0 °C
179000 psi
@Temperature 73.4 °F
Flexural Modulus 101.4 GPa
@Temperature 23.0 °C
14710 ksi
@Temperature 73.4 °F
Compressive Yield Strength 1517 MPa
@Temperature 23.0 °C
220000 psi
@Temperature 73.4 °F
Compressive Modulus 121 GPa
@Temperature 23.0 °C
17500 ksi
@Temperature 73.4 °F
Shear Strength 90.0 MPa
@Temperature 23.0 °C
13100 psi
@Temperature 73.4 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Epoxy, Cast, Unreinforced
DuPont™ Kevlar® 49 Aramid Fiber
DuPont™ Kevlar® 29 Aramid Fiber
Hexcel® HexForce™ X8T196 Carbon Fabric
Hexcel® HexPly® ES70 120°C Curing Epoxy Matrix, E-glass UD fabric 430 g/m2

PHEXC131 / 98601

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.