MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Syensqo (Solvay Specialty Polymers) Amodel® ET-1001 HS Polyphthalamide (PPA) Resin, Dry As Molded  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), High Impact

Material Notes: AMODEL ET-1001 HS resin is an impact modified polyphthalamide (PPA) with exceptional impact strength and practical toughness. AMODEL PPA resins offer high fatigue strength, and good chemical resistance combined with good mechanical property retention over a broad temperature/humidity range. Possible applications for AMODEL ET-1001 HS resin include: anti-friction and wear resistant components, and components of chemical and oil processing equipment, sporting goods, automobiles, household appliances, power tools, and safety equipment, where exceptional impact strength and high modulus are required. AMODEL ET-1001 HS resin contains a lubricant for easier processing with conventional equipment and methods. This grade is also heat stabilized for better performance at high temperatures.

This product line was acquired by Solvay Advanced Polymers from BP Amoco in November 2001.

MatWeb has an entry for this material conditioned at 50% RH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³ASTM D792
Water Absorption 0.65 %0.65 %24 hrs. ASTM D570
Linear Mold Shrinkage 0.020 cm/cm0.020 in/inASTM E831
Linear Mold Shrinkage, Transverse 0.020 cm/cm0.020 in/inASTM E831
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 76.0 MPa11000 psiASTM D638
Elongation at Break 30 %30 %ASTM D638
Elongation at Yield 6.0 %6.0 %ASTM D638
Tensile Modulus 2.40 GPa348 ksiASTM D638
Flexural Yield Strength 128 MPa18600 psiASTM D790
Flexural Modulus 2.60 GPa377 ksiASTM D790
Poissons Ratio 0.350.35
Shear Modulus 0.889 GPa129 ksiCalculated
Izod Impact, Notched 9.60 J/cm18.0 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 310 °C590 °FASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 120 °C248 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 321 - 343 °C610 - 649 °FInjection

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Amodel® ET-1001 L Polyphthalamide (PPA) Resin, Dry as Molded
Aluminum, Al
Syensqo (Solvay Specialty Polymers) Amodel® ET-1001 L Polyphthalamide (PPA) Resin, at 50% RH

PSOLVT47 / 21343

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.