MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Vycom Corzan® CPVC Chlorinated PVC
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Corzan CPVC is a high heat, corrosion resistant chlorinated polyvinyl chloride (CPVC) sheet. Because of its excellent corrosion resistance at elevated temperatures, it is ideally suited for self-supporting constructions where high temperatures are a concern. It can be used (depending on chemistry) up to 180º F. Corzan CPVC conforms to ASTM-D-1784-95 Class 23447-B (formerly Type IV Grade 1) and is manufactured without fillers or plasticizers.

FEATURES AND BENEFITS

  • System compatibility- Corzan is available in pipe, valves, fitting and sheet to construct completely compatible systems.
  • Machinable- Corzan can be machined, cut, routed and welded.
  • Flammability- Corzan is self extinguishing and has a flame spread of less than 20.
  • Physical properties- Corzan has outstanding strength through a range of temperatures.
  • Impact- Corzan has excellent impact strength.
  • Chemical resistance- Corzan has excellent chemical resistance to acids and alkalis.

Information provided by Compression Polymers Corp - Vycom

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.47 g/cc0.0531 lb/in³ASTM D792
Water Absorption 0.030 %0.030 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 116116ASTM D785
Tensile Strength, Ultimate 50.3 MPa7300 psiASTM D638
Flexural Strength 98.6 MPa14300 psiASTM D790
Flexural Modulus 2.49 GPa361 ksiASTM D790
Compressive Strength 69.6 MPa10100 psiASTM D695
Compressive Modulus 1.35 GPa196 ksiASTM D695
Izod Impact, Notched 4.81 J/cm9.00 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.40e+15 ohm-cm3.40e+15 ohm-cmASTM D257
Dielectric Constant 3.7
@Frequency 60 Hz
3.7
@Frequency 60 Hz
ASTM D150
Dielectric Strength 49.2 kV/mm1250 kV/inASTM D147
Dissipation Factor 0.000070
@Frequency 1000 Hz
0.000070
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 69.5 µm/m-°C
@Temperature 20.0 °C
38.6 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Thermal Conductivity 0.140 W/m-K0.972 BTU-in/hr-ft²-°FASTM C177
Deflection Temperature at 1.8 MPa (264 psi) 92.2 °C198 °FASTM D648
Flammability, UL94 5VB
@Thickness 1.57 mm
5VB
@Thickness 0.0620 in
Flame Spread Index 1515ASTM E84
Oxygen Index 60 %60 %ASTM D2863
 
Descriptive Properties
Cell Class24446-BASTM D1784
Smoke Developed70 to 125ASTM E84

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Axiall ProTherm® 4526 CPVC Rigid PVC, Molding
Overview of materials for Chlorinated PVC (CPVC)
Vycom FLAMETEC™ CPVC Chlorinated Polyvinyl Chloride Sheet
Geon® Performance Solutions CPVC LC500 Polyvinyl Chloride, Chlorinated (CPVC)
Westlake Plastics Corzan® II CPVC Sheet

PCPCV01 / 29073

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.