MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Polychloroprene Rubber (CR)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Polychloroprene rubber usually withstands ozone, oli/fat/grease, and many solvents. It is impacted by esters, ketones, chlorinated solvents, aromatic hydrocarbons, strong oxidizing acids, and nitrogen containing hydrocarbons.

Key Words: Trade Name: Neoprene
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.35 - 1.50 g/cc0.0488 - 0.0542 lb/in³Compounded
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 35 - 9535 - 95Depends on compounding
Tensile Strength, Ultimate 28.0 MPa4060 psiCompounded Tire
Elongation at Break 100 - 800 %100 - 800 %
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 100 °C212 °F
Minimum Service Temperature, Air -30.0 °C-22.0 °F

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Armacell Monarch® F-02001 Neoprene Based Rubber Foam
Cos40 Cork/Neoprene Rubber Sheet
DuPont Mobility and Materials Neoprene FB Polychloroprene Rubber
Nitrile Rubber (NBR, Acrylonitrile-Butadiene Rubber)
Denka Neoprene 671A Polychloroprene

P0RU13 / 20061

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.