MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

DuPont Teijin Films Melinex® 516 Polyester Film
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Melinex® 516 is a high clarity polyester film which is pretreated on both sides for slip to combine good handling properties with high clarity and brilliance.

Typical Applications: Some typical uses include: layout base, post lamination, MTS, color proofing, labels, flexible circuits, archival sheeting, and printing plates.

Approvals: UL 94 VTM-2 - for 300 - 700 gauge (0.076 - 0.18mm) and Library of Congress Specification - This film meets the Library of Congress Specification Number 500-500-5/31/95 for use in archival storage.

Available in 250, 275, 300, 360, 370, 400, 460, 500, and 600 Gauge

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 96.5 MPa14000 psiASTM D882A
Film Tensile Strength at Yield, TD 100 MPa14500 psiASTM D882A
Film Elongation at Break, MD 180 %180 %ASTM D882A
Film Elongation at Break, TD 120 %120 %ASTM D882A
Coefficient of Friction, Dynamic 0.450.45A-B; ASTM D1894
Film Tensile Strength at Break, MD 193 MPa28000 psiASTM D882A
Film Tensile Strength at Break, TD 241 MPa35000 psiASTM D882A
 
Thermal PropertiesMetricEnglishComments
Shrinkage, MD 2.5 %
@Temperature 190 °C,
Time 300 sec
2.5 %
@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 0.40 %
@Temperature 190 °C,
Time 300 sec
0.40 %
@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
 
Optical PropertiesMetricEnglishComments
Transmission, Visible  88 %
@Thickness 0.127 mm
88 %
@Thickness 0.00500 in
TLT; ASTM D1003
 88.3 %
@Thickness 0.102 mm
88.3 %
@Thickness 0.00400 in
TLT; ASTM D1003
 88.5 %
@Thickness 0.0673 mm
88.5 %
@Thickness 0.00265 in
TLT; ASTM D1003
 88.5 %
@Thickness 0.0762 mm
88.5 %
@Thickness 0.00300 in
TLT; ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Teijin Films Melinex® 487 Polyester Film, 200 Gauge
DuPont Teijin Films Melinex® 478 Polyester Film, 200 Gauge
DuPont Teijin Films Melinex® 475 Polyester Film, 200 Gauge
DuPont Teijin Films Melinex® 505 Polyester Film
DuPont Teijin Films Melinex® 513P Polyester Film, 650 Gauge

PDTZ9132 / 139500

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.