MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

ExxonMobil LL 5100.09 LLDPE Master Batch Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: Linear low-density polyethylene (LLDPE) resins are used to produce a wide range of products. They are commonly processed neat or in blends with LDPE and/or HDPE.  Benefits: Versatile and cost effective, Lower seal initiation temperature balanced with mechanical properties, Can reduce costs in high-performance structures.  LL 5100.09 is a LLDPE resin deigned to provide good processability and ease of blending.  The granular form of LL 5100.09 make for efficient blending with pigments, slip and antiblock additives. 

Availability:  Latin America, North America. 

Additive:  antiblock: no; processing aid: no; slip: no; thermal stabilizer: yes. 

Applications:  Master batch base resin.  Forms:  granules.

Information provided by ExxonMobil.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.925 g/cc0.0334 lb/in³ASTM D1505
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 190 °C
20 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 50
@Time 15.0 sec
50
@Time 0.00417 hour
ASTM D2240
Tensile Strength at Break 7.58 MPa1100 psiASTM D638
Tensile Strength, Yield 14.5 MPa2100 psiASTM D638
Elongation at Break 60 %60 %ASTM D638
Flexural Modulus, 1% Secant 427 MPa62000 psiASTM D790
Izod Impact, Notched 5.34 J/cm10.0 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 122 °C252 °FPeak; ExxonMobil Method
Brittleness Temperature <= -76.1 °C<= -105 °FASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Purell 2410T Linear Low Density Polyethylene (LLDPE), Blow Molding Grade
Versalis Flexirene® MR 50 U Linear Low Density Polyethylene
Versalis Flexirene® MR 50 A Linear Low Density Polyethylene
ICO Polymers ICOFLO™ 510-5069 400 Micron LLDPE Powder
Graft Polymer GRAFTAPOR™ LL-S 02050 Porous Linear Low Density Polyethylene Carrier

PEX98859 / 238241

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.