MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Zirconium Oxide, Zirconia, ZrO2
Categories: Ceramic; Oxide; Zirconium Oxide

Material Notes: White amorphous powder.

Property data is listed for pure zirconia. Commercial zirconia ceramics contain additions of components such as yttrium oxide, calcium oxide, or magnesium oxide to stabilize the high temperature zirconia phase and prevent transformation to the room temperature stable monoclinic phase.

Key Words: Zirconium Oxide, ZrO2
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 5.68 g/cc0.205 lb/in³monoclinic
 6.10 g/cc0.220 lb/in³tetragonal
Molecular Weight 123.223 g/mol123.223 g/mol
 
Electrical PropertiesMetricEnglishComments
Magnetic Susceptibility -0.0000138-0.0000138cm^3/mol
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 706 J/g304 BTU/lb
CTE, linear  7.00 µm/m-°C
@Temperature 20.0 °C
3.89 µin/in-°F
@Temperature 68.0 °F
monoclinic
 12.0 µm/m-°C
@Temperature 20.0 °C
6.67 µin/in-°F
@Temperature 68.0 °F
tetragonal
Thermal Conductivity 1.675 W/m-K11.62 BTU-in/hr-ft²-°Fmonoclinic
Melting Point 2681 - 2847 °C4858 - 5157 °F

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Yttria Stabilized Zirconia, YSZ
Magnesia Stabilized Zirconia
Corundum, Aluminum Oxide, Alumina, 99.9%, Al2O3
MarkeTech Zirconium Oxide Ceramic, Zirconia MgO Stabilized
MarkeTech Zirconium Oxide Ceramic - Zirconia, Y2O3 Stabilized

BOZrA / 284

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.