MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

A. Schulman BMC A50-XHS High Strength Grade Molding Compound
Categories: Polymer; Thermoset; Polyester, TS; Polyester (Thermoset) - Rigid

Material Notes: BMC A50-XHS is a high strength bulk molding compound. Due to the excellent flow and controlled reactivity, BMC A50-XHS is well suited for injection, transfer or compression molding. Typical applications are circuit breakers, light housings and structural parts.

Information provided by Bulk Molding Compounds, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.79 - 1.85 g/cc0.0647 - 0.0668 lb/in³Molded
Linear Mold Shrinkage 0.0015 - 0.0032 cm/cm0.0015 - 0.0032 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 30 - 5030 - 50
Tensile Strength 57.2 - 71.0 MPa8300 - 10300 psi
Flexural Strength 124 - 152 MPa18000 - 22000 psi
Flexural Modulus 11.7 - 13.1 GPa1700 - 1900 ksi
Compressive Strength 116 - 143 MPa16800 - 20800 psi
Izod Impact, Notched 5.34 - 6.41 J/cm10.0 - 12.0 ft-lb/in
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 14.8 - 16.7 kV/mm375 - 425 kV/inshort time
Arc Resistance >= 186 sec>= 186 sec
Comparative Tracking Index >= 500 V>= 500 V
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C>= 500 °F
Flammability, UL94 V-0V-0UL 94 V0/UL 94 5V
 
Processing PropertiesMetricEnglishComments
Processing Temperature 138 - 166 °C280 - 330 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
G-10 Fiberglass Epoxy Laminate Sheet
A. Schulman BMC 685 Mineral Filled, Glass Fiber Reinforced Polyester Compound
Covestro Bayblend® FR3005 BBS310 PC/ABS Blend
A. Schulman BMC 695 Vinyl Ester Molding Compound
Covestro Bayblend® FR3006 HF PC/ABS Blend

PBMC914 / 123378

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.