MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

DuPont Mobility and Materials Kalrez® 6375UP FFKM Perfluoroelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Resists chemical attack and is formulated and processed to minimize the potential for undesirable contaminants. Kalrez® 6375UP has the best balance of performance characteristics required for semicon wet processing environments.

Information provided by manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.99 g/cc0.0719 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7575ASTM D 2240
Elongation at Break 160 %160 %ASTM D 412
100% Modulus 9.10 MPa1320 psiASTM D 412
Compression Set  24 %
@Temperature 204 °C,
Time 252000 sec
24 %
@Temperature 399 °F,
Time 70.0 hour
Pellet (Type 1); ASTM D 395B
 25 %
@Temperature 204 °C,
Time 252000 sec
25 %
@Temperature 399 °F,
Time 70.0 hour
O-ring (AS568-214); ASTM D 1414
 
Thermal PropertiesMetricEnglishComments
CTE, linear 289 µm/m-°C161 µin/in-°FISO 11359-1/-2
Maximum Service Temperature, Air 275 °C527 °FDuPont proprietary test
Minimum Service Temperature, Air -20.0 °C-4.00 °FDuPont proprietary test
 -3.00 °C26.6 °FRetraction temperature TR-10; ASTM D 1329
 
Descriptive Properties
ColorBlack
Polymer(FFKM)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Kalrez® 6221 FFKM Perfluoroelastomer
DuPont Mobility and Materials Kalrez® 8575 FFKM Perfluoroelastomer
DuPont Mobility and Materials Kalrez® 6375 FFKM Perfluoroelastomer
DuPont Mobility and Materials Kalrez® 4079 FFKM Perfluoroelastomer
DuPont Mobility and Materials Kalrez® 6230 FFKM Perfluoroelastomer

PDVD056 / 33875

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.