System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Kazanorgsintez 271-274K Cable Composition Based on High Density Polyethylene
Categories:
Polymer
;
Thermoplastic
;
Polyethylene (PE)
;
High Density (HDPE)
Material Notes:
Production Method:
Gaseous-phase method.
Application:
Compositions are intended for cover insulating lapping, protective covers and cables.
Information Provided by Kazanorgsintez
Key Words:
HDPE
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
0.950
-
0.955
g/cc
0.0343
-
0.0345
lb/in³
Volatiles
<= 0.000010 %
<= 0.000010 %
Superior Class
<= 0.000015 %
<= 0.000015 %
1st Class
Environmental Stress Crack Resistance
>=
500
hour
>=
500
hour
Melt Flow
0.30
-
0.65
g/10 min
@Load 5.00 kg
0.30
-
0.65
g/10 min
@Load 11.0 lb
±10% Superior Class, ±15% 1st Class
Ash
<= 0.050 %
<= 0.050 %
Superior Class
<= 0.075 %
<= 0.075 %
1st Class
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
>=
22.6
MPa
>=
3280
psi
Elongation at Break
>= 700 %
>= 700 %
Tear Strength Test
>= 21.6
>= 21.6
MPa
Electrical Properties
Metric
English
Comments
Dielectric Constant
<= 2.4
@Frequency 1000 Hz
<= 2.4
@Frequency 1000 Hz
Dielectric Strength
>=
35.0
kV/mm
@Frequency 50 Hz
>=
889
kV/in
@Frequency 50 Hz
Sample of 1 mm thickness, Alternating current
Dissipation Factor
<= 0.00020
@Frequency 1000 Hz
<= 0.00020
@Frequency 1000 Hz
Thermal Properties
Metric
English
Comments
Maximum Service Temperature, Air
200
°C
@Time >=1200 sec
392
°F
@Time >=0.333 hour
Descriptive Properties
Amount of impurities [pcs]
10
Superior Class
20
1st Class
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
EPICHEM Epilen PP 20GF NAT Polypropylene, 20% Glass Fiber
Premix Thermoplastics PREBLACK PP 704-35 Polypropylene, 35% Carbon Black
Polyram RamLloy PB917G6 Nylon 6/Polypropylene Alloy, 30% Glass Fiber Reinforced
Overview of materials for Polypropylene with 20% Glass Fiber Filler
Premix Thermoplastics PREADD FIB 5551
PKAZAN038 / 127357
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.