MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Visit Zeus Inc. for PEEK Tubing

Search Results

The search phrase you entered, low carbon steel, is common to 1612 materials, by searching on the exact phrase [ "low carbon steel" ] in the most common text fields.

Results are displayed up to a maximum of 200 materials per page. Follow the links below to view complete property information. If your material is not listed, please refer to our search help page for assistance in limiting your search.

Expand Search Results
By clicking on the "Broaden" button, MatWeb will continue to modify your search criteria in an effort to provide you with a better result set. Your search terms may be modified in the following ways: 1) We will search additional text fields    2) We will add conjunctions "AND" or "OR" between individual words (for multiple words)   3) We will search terms using wildcards (as if they are prefixes or suffixes) of individual words


Found 1612 Results -- Page of 33 -- [Prev Page] [Next Page] --  view per page
Use Folder Contains  
Select Material Name
 1Overview of materials for Low Carbon Steel
 2AISI 1005 Steel
 3AISI 1006 Steel, cold drawn
 4AISI 1006 Steel, hot rolled bar, 19-32 mm (0.75-1.25 in) round
 5AISI 1006 Steel, cold drawn bar, 19-32 mm (0.75-1.25 in) round
 6AISI 1006 Steel, CQ, DQ, and DQSK sheet, 1.6-5.8 (0.06-0.23 in) mm thick
 7AISI 1008 Steel, hot rolled bar, 19-32 mm (0.75-1.25 in) round
 8AISI 1008 Steel, cold drawn bar, 19-32 mm (0.75-1.25 in) round
 9AISI 1008 Steel, CQ, DQ, and DQSK sheet, 1.6-5.8 mm thick
 10AISI M1008 Merchant Quality Carbon Steel, Composition Spec
 11DiscontinuedAISI 1009 Steel
 12AISI 1010 Steel, cold drawn
 13AISI 1010 Steel, hot rolled bar, 19-32 mm (0.75-1.25 in) round or thickness
 14AISI 1010 Steel, cold drawn bar, 19-32 mm (0.75-1.25 in) round or thickness
 15AISI 1010 Steel, CQ sheet,1.6-5.8 mm round or thickness
 16AISI M1010 Merchant Quality Carbon Steel, Composition Spec
 17AISI 1012 Steel, cold drawn
 18AISI 1012 Steel, hot rolled bar, 19-32 mm (0.75-1.25 in) round or thickness
 19AISI 1012 Steel, cold drawn bar, 19-32 mm (0.75-1.25 in) round or thickness
 20AISI 1012 Steel, CQ sheet,1.6-5.8 mm round or thickness
 21AISI M1012 Merchant Quality Carbon Steel, Composition Spec
 22AISI 1013 Carbon Steel Composition Spec
 23AISI 1015 Steel, cold drawn
 24AISI 1015 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round
 25AISI 1015 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
 26AISI 1015 Steel, as rolled
 27AISI 1015 Steel, normalized at 925°C (1700°F)
 28AISI 1015 Steel, annealed at 870°C (1600°F)
 29AISI 1015 Steel, annealed at 870°C (1600°F), furnace cooled 17°C (31°F) per hour to 725°C (1340°F), air cooled, 25 mm (1 in.) round
 30AISI 1015 Steel, normalized at 925°C (1700°F), 13 mm (0.5 in.) round
 31AISI 1015 Steel, normalized at 925°C (1700°F), 25 mm (1 in.) round
 32AISI 1015 Steel, normalized at 925°C (1700°F), 50 mm (2 in.) round
 33AISI 1015 Steel, normalized at 925°C (1700°F), 100 mm (4 in.) round
 34AISI 1015 Steel, mock carburized at 915°C (1680°F) for 8 hours, 775°C (1430°F) reheat, water quenched, 175°C (350°F) temper, 13 mm (0.5 in.) round
 35AISI 1015 Steel, mock carburized at 915°C (1680°F) for 8 hours, 775°C (1430°F) reheat, water quenched, 175°C (350°F) temper, 25 mm (1 in.) round
 36AISI 1015 Steel, mock carburized at 915°C (1680°F) for 8 hours, 775°C (1430°F) reheat, water quenched, 175°C (350°F) temper, 50 mm (2 in.) round
 37AISI 1015 Steel, mock carburized at 915°C (1680°F) for 8 hours, 775°C (1430°F) reheat, water quenched, 175°C (350°F) temper, 100 mm (4 in.) round
 38AISI M1015 Merchant Quality Carbon Steel, Composition Spec
 39AISI 1016 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round
 40AISI 1016 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
 41AISI 1017 Steel, cold drawn
 42AISI 1017 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
 43AISI M1017 Merchant Quality Carbon Steel, Composition Spec
 44AISI 1018 Steel, cold drawn
 45AISI 1018 Steel, hot rolled, quenched, and tempered
 46AISI 1018 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
 47AISI 1018 Steel, cold drawn, quenched, and tempered, 19-32 mm (0.75-1.25 in) round
 48AISI 1018 Steel, as cold drawn, 16-22 mm (0.625-0.875 in) round
 49AISI 1018 Steel, as cold drawn, 22-32 mm (0.875-1.25 in) round
 50AISI 1018 Steel, as cold drawn, 32-50 mm (1.25-2 in) round
 
Found 1612 Results -- Page of 33 -- [Prev Page] [Next Page] --  view per page

Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.


Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.