MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Proto3000 – 3D Engineering Solutions

Search Results

The search phrase you entered, 17-4ph, is common to 40 materials, by searching on the term(s) [ "17-4ph" ] in most common text fields, .

Results are displayed up to a maximum of 200 materials per page. Follow the links below to view complete property information. If your material is not listed, please refer to our search help page for assistance in limiting your search.

Expand Search Results
By clicking on the "Broaden" button, MatWeb will continue to modify your search criteria in an effort to provide you with a better result set. Your search terms may be modified in the following ways: 1) We will search additional text fields    2) We will add conjunctions "AND" or "OR" between individual words (for multiple words)   3) We will search terms using wildcards (as if they are prefixes or suffixes) of individual words


Found 40 Results -- Page of 1 -- [Prev Page] [Next Page] --  view per page
Use Folder Contains  
Select Material Name
 1Cast Stainless Steel 17- 4, UNS J92150 (Compostion Spec)
 2DiscontinuedLatitude Manufacturing PowderFlo® 17-4PH Stainless Steel Metal Injection Molding Compound
 3ATI Allvac® Vasco® 17-4 Precipitation Hardening Steel, Heat Treatment: 1038°C (1900°F) + Age
 4Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Annealed
 5Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1025 (Heated 552°C)
 6Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1075 (Heated 579°C)
 7Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1150 (Heated 621°C)
 8Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1150M (Heated 760°C/2hr/AC then 621°C/4hr/AC)
 9Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 900 (Age-Hardened 482°C/1hr/AC)
 10Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1100 (Heated 593°C)
 11EOS StainlessSteel 17-4PH DMSL on EOS M 290
 12ExOne 17-4PH Stainless Steel for 3D Printing
 13Industeel VIRGO 17.4PH 17Cr-4Ni-3Cu Precipitation Hardening Martensitic Stainless Steel (496°C - 4 hours + air cooled)
 14Industeel VIRGO 17.4PH 17Cr-4Ni-3Cu Precipitation Hardening Martensitic Stainless Steel (593°C - 4 hours + air cooled)
 15Industeel VIRGO 17.4PH 17Cr-4Ni-3Cu Precipitation Hardening Martensitic Stainless Steel (480°C (900°F) - 1 hour + air cooled)
 16Kinetics MIM 17-4PH Stainless Steel (As Sintered)
 17Kinetics MIM 17-4PH Stainless Steel (H900 Condition)
 18Kinetics MIM 17-4PH Stainless Steel (H1100 Condition)
 19ATI Allegheny Ludlum AL 17-4 High Strength Stainless Steel, UNS S17400
 20Ametek 17-4 P/M Process, Sintered at 2050°F (1121°C)
 21Ametek 17-4 P/M Process, Sintered at 2200°F (1204°C)
 22Ametek 17-4 P/M Process, Sintered at 2300°F (1260°C)
 23Sandvik Osprey 17-4 PH/MA Stainless Steel Master Alloy Powder (Grade 80% - 22)
 24Sandvik Osprey 17-4 PH/MA Stainless Steel Master Alloy Powder (Grade 90% - 22)
 25Sandvik Osprey 17-4 PH/MA Stainless Steel Master Alloy Powder (Grade 90% - 16)
 26Sandvik Osprey 17-4 PH/MA Stainless Steel Master Alloy Powder (Grade 95% - 16)
 27Sandvik Osprey 17-4 PH Stainless Steel Powder (Grade 80% - 22)
 28Sandvik Osprey 17-4 PH Stainless Steel Powder (Grade 90% - 22)
 29Sandvik Osprey 17-4 PH Stainless Steel Powder (Grade 90% - 16)
 30Sandvik Osprey 17-4 PH Stainless Steel Powder (Grade 95% - 16)
 31Proto Labs 17-4PH Stainless Steel - DMLS
 32PSM Industries PolyAlloys MIM-17-4PH sintered Stainless Steel
 33PSM Industries PM Krupp 17-4PH Stainless Steel
 34FloMet 17-4 PH Stainless Steel, As Sintered
 35FloMet 17-4PH Stainless Steel, Heat Treated (H-900)
 363D Systems LaserForm® 17-4PH (B) Stainless Steel Materials
 373D Systems LaserForm® 17-4PH (A) AS-BUILT Stainless Steel Material
 383D Systems LaserForm® 17-4PH (A) H900 Stainless Steel Material
 393D Systems LaserForm® 17-4PH (A) H1150 Stainless Steel Material
 40Matexcel MET-0009 GP1 (17-4PH) Stainless steel Powder
 
Found 40 Results -- Page of 1 -- [Prev Page] [Next Page] --  view per page

Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.


Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.