MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
Aluminum 6061-O  (Unverified Data**)
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 6000 Series Aluminum Alloy

Material Notes: Information provided by Alcoa and the references. General 6061 characteristics and uses: Excellent joining characteristics, good acceptance of applied coatings.

Key Words: al6061, UNS A96061; ISO AlMg1SiCu; Aluminium 6061-O, AD-33 (Russia); AA6061-O; Al6061-O
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.70 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 30500 kg load with 10 mm ball
Tensile Strength, Ultimate 125 MPa
Tensile Strength, Yield 55.0 MPa
Elongation at Break 25 %
@Thickness 1.60 mm
in 5 cm
Modulus of Elasticity 69.0 GPaAverage of Tension and Compression. In Aluminum alloys, the compressive modulus is typically 2% greater than the tensile modulus
Ultimate Bearing Strength 228 MPaEdge distance/pin diameter = 2.0
Bearing Yield Strength 103 MPaEdge distance/pin diameter = 2.0
Poissons Ratio 0.33Estimated from trends in similar Al alloys.
Fatigue Strength 60.0 MPa
@# of Cycles 5.00e+8
Machinability 30 %0-100 Scale of Aluminum Alloys
Shear Modulus 26.0 GPaEstimated from similar Al alloys.
Shear Strength 80.0 MPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000370 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 23.6 µm/m-°C
@Temperature 20.0 - 100 °C
 25.2 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.896 J/g-°C
Thermal Conductivity 180 W/m-K
Melting Point 582 - 652 °C
Solidus 582 °C
Liquidus 652 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 98 %As remainder
Chromium, Cr 0.040 - 0.35 %
Copper, Cu 0.15 - 0.40 %
Iron, Fe <= 0.70 %
Magnesium, Mg 0.80 - 1.2 %
Manganese, Mn <= 0.15 %
Silicon, Si 0.40 - 0.80 %
Titanium, Ti <= 0.15 %
Zinc, Zn <= 0.25 %

References for this datasheet.

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MA6010 / 9341

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.