MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

ExxonMobil Optema® TC-113 Ethylene Methyl Acrylate for Compounding  (discontinued **)
Categories: Polymer; Thermoplastic; Ethylene Methyl Acrylate; Ethylene-Methyl Acrylate Copolymer, Compounding Grade

Material Notes: Data provided by the manufacturer, Exxon Chemical.

23.5% Methyl Acrylate. An Ethylene Methyl Acrylate copolymer which can be used as an impact modifier or compatibilizer in polymer compounds. It can also be used in coextrusions where adhesion and thermal processing stability are required or as an elastic, tough monolayer film.

Applications: Compatibilizer and impact modifier for engineering thermoplastics; Coextruded tie layer for flexible packaging applications.

Key Words: EMA; Exxon Chemical Company
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.939 g/cc0.0339 lb/in³Exxon Method
Melt Flow 1.0 g/10 min1.0 g/10 minExxon Method
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8383ASTM D2240
Hardness, Shore D 3333ASTM D2240
Tensile Strength, Ultimate 11.0 MPa1600 psiASTM D638
Elongation at Break >= 800 %>= 800 %ASTM D638
Flexural Modulus 0.0260 GPa3.77 ksiASTM D790
Tensile Impact Strength 650 kJ/m²309 ft-lb/in²23°C; ASTM D-1822
 
Thermal PropertiesMetricEnglishComments
Melting Point 74.0 °C165 °FExxon Method
Vicat Softening Point 50.0 °C122 °F1000g; ASTM D-1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Optema® TC-221 Ethylene Methyl Acrylate for Compounding
DuPont Nucrel® 535 Ethylene-Methacrylic Acid Copolymer Resin
DuPont Nucrel® 2940 Ethylene-Methacrylic Acid Copolymer Resin
DuPont Nucrel® 2906 Ethylene-Methacrylic Acid Copolymer Resin
Dow Nucrel® 960 Ethylene-Methacrylic Acid Copolymer Resin

PEXCEW / 37908

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.