MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

BASF Ultramid® C33 01 PA66/6 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, Unreinforced

Material Notes: Ultramid C33 01 is an intermediate viscosity PA6/66 grade. Its lower melting point than standard PA6 is advantageous for coextrusion with temperature sensitive polymers like EVOH. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German BfR recommendation "X Polyamide", 1.6.1998 or legislations for other countries will be provided on request.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³ISO 1183
Water Absorption 10.5 %10.5 %ISO 62
Moisture Absorption at Equilibrium 3.2 %3.2 %23°C/50% R.H.; ISO 62
Relative Viscosity 3.3 cP3.3 cPISO Test; 96 % SAV
Viscosity Number 195 cm³/g1.95 dl/g
Linear Mold Shrinkage 0.010 cm/cm0.010 in/inASTM Data; MD
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 80.0 MPa11600 psi0.2 in/min; ASTM Test
Tensile Strength, Yield 80.0 MPa11600 psi50mm/min; ISO 527
Elongation at Break >= 50 %>= 50 %50mm/min, Nominal strain; ISO 527
Elongation at Yield 5.0 %5.0 %50mm/min; ISO 527
Tensile Modulus 2.20 GPa319 ksi1mm/min; ISO 527
 2.40 GPa348 ksiASTM Test
Charpy Impact Unnotched NBNBISO 179
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179
Charpy Impact, Notched NBNBISO 179
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+12 ohm1.00e+12 ohmIEC 60093
Dielectric Constant  3.7
@Frequency 100 Hz
3.7
@Frequency 100 Hz
IEC 60250
 3.7
@Frequency 1e+6 Hz
3.7
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor  0.030
@Frequency 1e+6 Hz
0.030
@Frequency 1e+6 Hz
IEC 60250
 0.030
@Frequency 100 Hz
0.030
@Frequency 100 Hz
IEC 60250
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 196 °C385 °F10 K/min
 196 °C385 °FASTM Test
Deflection Temperature at 0.46 MPa (66 psi) 140 °C284 °FASTM Test
 140 °C284 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 57.0 °C135 °FASTM Test
 57.0 °C135 °FISO 75
 
Compliance PropertiesMetricEnglishComments
FDA YesYes21 CFR 177.1500 (restrictions per 21 CFR .1395)
 
Descriptive Properties
ColorNatural
Commercial StatusNorth America and Europe
FormPellets
Impact ModifiedNo
Primary Processing TechniqueFilm Extrusion
ProcessingOther Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® C33 01 PA66/6 (Conditioned)
BASF Ultramid® C33L 01 PA66/6 (Dry)
DuPont Selar® PA 3426 Nylon Barrier Resin
Teknor Apex Chemlon 275 Nylon 6, Copolymer Impact Modified
BASF Ultramid® C40LX 01 PA66/6 (Conditioned)

PBASF9357 / 85121

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.