MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

NOVA Chemicals Sclair® FP020-D Octene Copolymer LLDPE Film Resin
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Octene, Film

Material Notes: FP020-D complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. FP020-D is subject to the specific limitation that it may contact food only at temperatures of 212°F and below.

NOVA Chemicals' polyethylene resins are chemically and biologically inert.

Features: Outstanding toughness and strength, Excellent sealability, Low gel

Additives: Antioxidant, Polymer process aid, Antiblock, Slip

Applications: Sealant and lamination film for food packaging, High strength film

Properties measured from blown film produced on a laboratory extruder with 4" die and a 35-mil die gap at a blowup ratio of 2.5:1, and melt temperature 420°F. Films were made from 100% FP020-D.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.921 g/cc0.0333 lb/in³ASTM D 792
Thickness 25.0 microns0.984 mil
Melt Flow 0.70 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.70 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 9.80 MPa1420 psiASTM D 882
Film Tensile Strength at Yield, TD 9.70 MPa1410 psiASTM D 882
Film Elongation at Break, MD 500 %500 %ASTM D 882
Film Elongation at Break, TD 800 %800 %ASTM D 882
Elmendorf Tear Strength MD 370 g370 gASTM D 1922
Elmendorf Tear Strength TD 650 g650 gASTM D 1922
Elmendorf Tear Strength, MD 14.8 g/micron376 g/milASTM D 1922
Elmendorf Tear Strength, TD 26.0 g/micron660 g/mil
Dart Drop Test 550 g1.21 lb22; ASTM D 1709/A
Film Tensile Strength at Break, MD 57.0 MPa8270 psiASTM D 882
Film Tensile Strength at Break, TD 46.0 MPa6670 psiASTM D 882
1% Secant Modulus, MD 180 MPa26100 psiASTM D 882
1% Secant Modulus, TD 205 MPa29700 psiASTM D 882
 
Optical PropertiesMetricEnglishComments
Haze 10 %10 %ASTM D 1003
Gloss 58 %58 %at 45°; ASTM D 2457
 
Descriptive Properties
Low Friction Puncture (J/mm)60NOVA Chemicals Test Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NOVA Chemicals Sclair® 11J4 Octene LLDPE Film Resin
NOVA Chemicals Sclair® 11J1 Octene LLDPE Film Resin
NOVA Chemicals Surpass® FPs117-C Octene Copolymer sLLDPE Film Resins
NOVA Chemicals Novapol® PF-0118-B Butene LLDPE Film Resin
NOVA Chemicals Novapol® PF-0118-D Butene LLDPE Film Resin

PNOV868 / 108475

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.