Kolon SPESIN® KP270EX Polybutylene Terephthalate (PBT)
Categories:
Polymer
;
Thermoplastic
;
Polyester, TP
;
Polybutylene Terephthalate (PBT)
;
Polybutylene Terephthalate (PBT), Extrusion Grade
Material Notes:
PBT, high viscosity, extrusion grade. General Purpose
Information provided by Kolon Plastic, Inc.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.31
g/cc
0.0473
lb/in³
ASTM D792
Water Absorption
0.080 %
@Time 86400 sec
0.080 %
@Time 24.0 hour
ASTM D570
Viscosity Number
160
cm³/g
1.6
dl/g
Phenol:1,2 Dichlorobenzene=1:1; ISO 1628-5
Melt Flow
8.0
-
12
g/10 min
@Load 2.16 kg,
Temperature 250 °C
8.0
-
12
g/10 min
@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
51.0
MPa
@Thickness 3.20 mm
7400
psi
@Thickness 0.126 in
50 mm/min; ASTM D638
Elongation at Break
>= 100 %
@Thickness 3.20 mm
>= 100 %
@Thickness 0.126 in
50 mm/min; ASTM D638
Flexural Strength
90.0
MPa
@Thickness 3.20 mm
13100
psi
@Thickness 0.126 in
5 mm/min; ASTM D790
Flexural Modulus
2.55
GPa
@Thickness 3.20 mm
370
ksi
@Thickness 0.126 in
5 mm/min; ASTM D790
Izod Impact, Notched
0.590
J/cm
@Thickness 6.40 mm,
Temperature 23.0 °C
1.11
ft-lb/in
@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties
Metric
English
Comments
Melting Point
224
°C
435
°F
20°C/min; ASTM D1525
Deflection Temperature at 0.46 MPa (66 psi)
60.0
°C
140
°F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
170
°C
338
°F
ASTM D648
Flammability, UL94
HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
Processing Properties
Metric
English
Comments
Rear Barrel Temperature
250
-
265
°C
482
-
509
°F
Middle Barrel Temperature
260
-
270
°C
500
-
518
°F
Front Barrel Temperature
260
-
270
°C
500
-
518
°F
Nozzle Temperature
260
-
275
°C
500
-
527
°F
Drying Temperature
100
-
120
°C
@Time 10800 - 18000 sec
212
-
248
°F
@Time 3.00 - 5.00 hour
Dehumidifying Dryer
Moisture Content
<= 0.040 %
<= 0.040 %
Descriptive Properties
Compression Ratio
3:1
Extruder (L/D)
24
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PKOKZ744 / 255755
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.