MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Lotte Advanced Materials Starex® GC-0770 H ABS/PET, Unreinforced Recycled  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; ABS Polymer; ABS/Polyester Alloy; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: Eco-friendly Post-Consumer recycled PET.

Information provided by Samsung Cheil Industries.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.09 g/cc1.09 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9595ASTM D785
Tensile Strength at Break 26.5 MPa3840 psi50 mm/min; ASTM D638
Tensile Strength, Yield 41.2 MPa5970 psi50 mm/min; ASTM D638
Elongation at Break 17 %17 %50 mm/min; ASTM D638
Tensile Modulus 1.77 GPa256 ksi50 mm/min; ASTM D638
Flexural Strength 49.0 MPa7110 psi2.8 mm/min; ASTM D790
Flexural Modulus 1.72 GPa249 ksi2.8 mm/min; ASTM D790
Izod Impact, Notched  1.96 J/cm
@Thickness 6.35 mm
3.67 ft-lb/in
@Thickness 0.250 in
ASTM D256
 4.41 J/cm
@Thickness 3.17 mm
8.27 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
@Thickness 6.40 mm
203 °F
@Thickness 0.252 in
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 83.0 °C
@Thickness 6.40 mm
181 °F
@Thickness 0.252 in
ASTM D648
Vicat Softening Point 90.0 °C194 °FB/50; ISO R306
 94.0 °C201 °FB/120; ISO R306

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lotte Advanced Materials Starex® EG-7000 ABS/PET, Unreinforced
Celanese Impet® 320R Recycled PET, 15% Glass Reinforced
Lotte Advanced Materials Starex® EG-7030 ABS/PET
Lotte Advanced Materials Starex® GC-0730 ABS/PET
INEOS Styrolution PS 116 N/L GPPS

PSAMSU738 / 146555

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.