MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Bakelite® PF 2774 Phenolic Molding Compound
Categories: Polymer; Thermoset; Phenolic; Phenolic, Novolac, Glass Filled

Material Notes: Phenolic molding compound, inorganically filled, glass fiber reinforced, increased dimensional stability, average notched impact strength, average heat resistance, improved electrical properties, UL listed molding compound 1.5 mm / V-0 (ALL).

Applications: MCB housings, pump parts, insulating flanges, automotive engine attachments

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.70 g/cc0.0614 lb/in³ISO 1183
Apparent Bulk Density 0.750 g/cc0.0271 lb/in³ISO 60
Linear Mold Shrinkage 0.0025 cm/cm0.0025 in/inCompression Molding. Post Shrinkage = 0.1%.; ISO 2577
 0.0040 cm/cm0.0040 in/inInjection Molding. Post Shrinkage = 0.2%.; ISO 2577
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 400 MPa58000 psiH961/30; ISO 2039/P1
Tensile Strength 65.0 MPa9430 psiISO 527 - 1/2
Tensile Modulus 10.0 GPa1450 ksiISO 527 - 1/2
Flexural Strength 110 MPa16000 psiISO 178
Flexural Modulus 11.0 GPa1600 ksiISO 178
Compressive Strength 225 MPa32600 psiISO 604
Charpy Impact Unnotched 0.850 J/cm²4.04 ft-lb/in²ISO 179-1 eU
Charpy Impact, Notched 0.240 J/cm²1.14 ft-lb/in²ISO 179-1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+12 ohm-cm1.00e+12 ohm-cm
Surface Resistance 1.00e+11 ohm1.00e+11 ohm
Dielectric Constant 7.5
@Frequency 100 Hz
7.5
@Frequency 100 Hz
Dielectric Strength 26.5 kV/mm
@Thickness 1.00 mm
673 kV/in
@Thickness 0.0394 in
IEC 60243-P1
Dissipation Factor 0.15
@Frequency 100 Hz
0.15
@Frequency 100 Hz
Comparative Tracking Index 175 V175 V
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 8.0 MPa 150 °C302 °FISO 75-2
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
All colors
 
Descriptive Properties
Water absorption (mg)1724h / 23°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bakelite® EP 8414 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage
Bakelite® UP 3420 Unsaturated Polyester Resin, High Mechanical Strength, High Arc Resistance, UL Listed, Low Shrinkage
Sumitomo Bakelite Durez® 152 Phenolic, Injection Grade
Sumitomo Bakelite Durez® 156 Phenolic, Injection Grade
Sumitomo Bakelite Durez® 118 Phenolic, Compression Grade

PBAKE984 / 192346

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.