MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

INEOS Styrolution Terblend® N NG-04 20% Glass Filled ABS/PA6 (Conditioned)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced; Nylon (Polyamide PA)

Material Notes: Terblend® N NG-04 is a 20% glass fiber reinforced ABS/PA blend with high dimensional stability and rigidity. Very high dimensional stability, Very high rigidity, High softening temperature. Applications: Automotive parts, Overhead consoles, Housings.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³dry; ISO 1183
Moisture Absorption at Equilibrium 1.1 %1.1 %beginning dry (23°C/50% R.H.); ISO 62
Melt Flow 11 g/10 min
@Load 10.0 kg,
Temperature 240 °C
11 g/10 min
@Load 22.0 lb,
Temperature 464 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 52.0 MPa7540 psi0.2 in/min; ASTM Test
Tensile Strength, Ultimate 60.0 MPa8700 psi5mm/min; ISO 527
Tensile Strength, Yield 54.0 MPa7830 psi2 in/min; ASTM Test
Elongation at Break 3.5 %3.5 %5mm/min; ISO 527
 5.0 %5.0 %0.2 in/min; ASTM Test
Tensile Modulus 3.59 GPa521 ksiASTM Test
 4.10 GPa595 ksi1mm/min; ISO 527
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+11 ohm-cm>= 1.00e+11 ohm-cmIEC 60093
Surface Resistance >= 1.00e+14 ohm>= 1.00e+14 ohmIEC 60093
Dielectric Constant  3.6
@Frequency 100 Hz
3.6
@Frequency 100 Hz
IEC 60250
 5.0
@Frequency 1e+6 Hz
5.0
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.050
@Frequency 1e+6 Hz
0.050
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 550 V550 VIEC 60112
 
Processing PropertiesMetricEnglishComments
Melt Temperature 265 °C509 °FInjection molding
Injection Velocity 65.0 mm/sec2.56 in/secInjection molding
 
Descriptive Properties
Commercial StatusActive America
Primary Processing TechniqueInjection Molding
UL.UL-CYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
INEOS Styrolution Terblend® N NG-04 20% Glass Filled ABS/PA6 (Dry)
INEOS Styrolution Terblend® N NM-19 ABS/PA6 (Conditioned)
INEOS Styrolution Terblend® N NG-02 EF 8% Glass Filled ABS+PA (Conditioned)
INEOS Styrolution Terblend® N NG-06 30% Glass Filled ABS/PA6 (Dry)
INEOS Styrolution Terblend® N NM-12 ABS/PA6 (Conditioned)

PBASF9035 / 84799

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.