MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Dow DOWLEX™ NG 2085 Linear Low Density Polyethylene, Ethylene-Octene Copolymer
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Octene, Film

Material Notes: Next Generation DOWLEX® NG 2085 resin is an ethylene-octene copolymer offering superior impact and tensile strength for down-gauged consumer liner film applications. It complies with U.S. FDA regulation 21 CFR 177.1520 c 3.2(a) for food contact applications. The regulation should be consulted for complete details.

Film properties below based on a film thickness of 25 µm. Data provided by Dow Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³
Thickness 25.0 microns0.984 mil
Melt Flow 0.95 g/10 min
@Load 2.16 kg
0.95 g/10 min
@Load 4.76 lb
Melt flow ratio I10/I2 is 8.
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 9.90 MPa1440 psi
Film Tensile Strength at Yield, TD 10.1 MPa1460 psi
Film Elongation at Break, MD 540 %540 %
Film Elongation at Break, TD 680 %680 %
Secant Modulus, MD 0.146 GPa21.2 ksiFilm value
Secant Modulus, TD 0.1545 GPa22.41 ksiFilm value
Elmendorf Tear Strength MD 350 g350 g
Elmendorf Tear Strength TD 665 g665 g
Elmendorf Tear Strength, MD 14.0 g/micron356 g/mil
Elmendorf Tear Strength, TD 26.6 g/micron676 g/mil
Dart Drop 29.0 g/micron737 g/mil
Film Tensile Strength at Break, MD 58.0 MPa8410 psi
Film Tensile Strength at Break, TD 46.0 MPa6670 psi
 
Processing PropertiesMetricEnglishComments
Processing Temperature 224 °C435 °FFilm extrusion temperature
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow DOWLEX™ NG 3347A Linear Low Density Polyethylene, Ethylene-Octene Copolymer
Dow DOWLEX™ 2032 Linear Low Density Polyethylene, Blown Film Grade
Dow DOWLEX™ 2056A Linear Low Density Polyethylene, Heavy Duty Film Grade
Dow DOWLEX™ 2085G Polyethylene Resin
Dow DOWLEX™ 2247G Polyethylene Resin

PDW467 / 34536

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.