MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

E-Polymers SEPAZ® V230A 30% Glass Fiber Reinforced PPA
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 30% Glass Fiber Reinforced

Material Notes: Polyphthal Amide Resin (High Temperature Nylon): SEPAZ PPA is a unique semi-crystalline engineering plastic that bridges the cost-performance gap between traditional engineering thermoplastics and super engineering thermoplastics. SEPAZ PPA resin has excellent mechanical properties (e.g. strength, stiffness, fatigue, creep resistance) over a broad temperature range. In addition to these, special grades formulated for applications requiring flame-retardancy, glycol-resistance, typically for automotive applications, and reflectivity, typically for optoelectronic applications such as high brightness LEDs, are available.

Information Provided by E-Polymers Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.46 g/cc1.46 g/ccASTM D792
Water Absorption 0.020 %
@Time 86400 sec
0.020 %
@Time 24.0 hour
Linear Mold Shrinkage 0.0020 cm/cm0.0020 in/in
Linear Mold Shrinkage, Transverse 0.0070 cm/cm0.0070 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 186.39 MPa27034 psiASTM D638
Elongation at Break 2.0 %2.0 %ASTM D638
Flexural Strength 255.06 MPa36993 psiASTM D790
Flexural Modulus 10.30 GPa1494 ksiASTM D790
Izod Impact, Notched 0.883 J/cm1.65 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 260 °C500 °FASTM D648
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Melt Temperature 300 - 330 °C572 - 626 °F
Mold Temperature 135 - 160 °C275 - 320 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lotte Advanced Materials Infino® TK-6036H PPA, Glass Filled
RTP Company RTP 4099 X 128640 Polyphthalamide (PPA), Thermally Conductive - Electrically Conductive - Preliminary Datasheet
RTP Company RTP 4099 X 131005 B Polyphthalamide (PPA), Thermally Conductive - Electrically Conductive
Syensqo (Solvay Specialty Polymers) Amodel® A-1133 L WH 015 Polyphthalamide (PPA), 33% Glass Fiber
Akro-Plastic Akromid® T1 GF 30 (3466) PPA Dry, 30% Glass Filled

PEPOLZ073 / 103570

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.