MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Iran Petrochemical (PCC) LL22501 Linear Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Blow Molding Grade

Material Notes: 22501 is a high stiffness LLDPE blown film grade designed for applications requiring good optical properties even at low extrusion temperature. This resin combines ease of processing with low gels and it is well suited for blending with LDPE and for general purpose application.

Information provided by Iran Petrochemical Commercial Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.922 g/cc0.0333 lb/in³ASTM D1505
Melt Flow 0.95 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.95 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 13.0 MPa1890 psiASTM D882
Film Tensile Strength at Yield, TD 12.5 MPa1810 psiASTM D882
Film Elongation at Break, MD 680 %680 %ASTM D882
Film Elongation at Break, TD 780 %780 %ASTM D882
2% Secant Modulus 0.200 GPa29.0 ksiMD; ASTM D882
 0.240 GPa34.8 ksiTD; ASTM D882
Elmendorf Tear Strength MD 105 g105 gASTM D1922
Elmendorf Tear Strength TD 460 g460 gASTM D1922
Dart Drop Test 80.0 g0.176 lbASTM D1709
Film Tensile Strength at Break, MD 45.0 MPa6530 psiASTM D882
Film Tensile Strength at Break, TD 30.0 MPa4350 psiASTM D882
 
Optical PropertiesMetricEnglishComments
Haze 21 %21 %ASTM D1003
Gloss 38 %38 %ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Iran Petrochemical (PCC) MF3820 High Density Polyethylene
Iran Petrochemical (PCC) Moplen Z 30 S Polypropylene
Iran Petrochemical (PCC) Moplen Z 30 G Polypropylene
Iran Petrochemical (PCC) EX 5 HM 9450 F High Density Polyethylene
Iran Petrochemical (PCC) LS0085/KJ Low Density Polyethylene

PIPC271 / 149733

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.