Data provided by the manufacturer, Exxon Chemical. An ethylene-based hexene plastomer produced using Exxon Chemical's EXXPOL technology. It is designed for monolayer and coextrusion coating industrial fill applications and cast films. Data for film properties below based on 0.8 mil film. |