16 mm ACRYLITER Resist high impact acrylic double-skin sheet is a light transmitting, heat-insulating and weatherresistant sheet made of impact-modified acrylic (polymethyl methacrylate, PMMA) polymer. 16 mm ACRYLITER Resist high impact acrylic double-skin sheet is suitable for sloped, curved and vertical applications including the following:- Canopies
- Carports
- Clerestory Glazing
- Interior Walls
- Interior Partitions
- Lighting Panels
- Conservatories
- Skylights
- Barrel Vaults
- Facades & Cladding
- Greenhouses
- Pool Enclosures
- Patio Covers
- Sunrooms
Advantages of 16 mm ACRYLITE® Resist high impact acrylic double-skin sheet- Extraordinary clear sheet is UV-resistant and includes a 30-year warranty against yellowing.
- Is coated with a completely non-toxic biologically neutral Anti Algae Application
- Offers excellent protection against excessive amounts of UV radiation.
- Up to 50% energy savings and minimizes CO2 emissions.
- Hail-resistant with a 10-year guarantee for withstanding hailstones with a kinetic energy of 1 joule.
- High light transmission in the PAR and visible spectral energy wavelengths.
- Impact resistance during transportation, handling and installation.
- Available in clear and a range of colors and solar tints.
Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm (Roehm) GmbH. |