MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Zhejiang Juner PA-A6-6H High CTI Value Halogen-Free Environmental Protection Flame-Resistant and Reinforced Polyamide
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Mineral Reinforced, Impact Grade

Material Notes: Applications: Circuit Breaker, Base

Information provided by Zhejiang Juner New Materials Co, Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.55 g/cc0.0560 lb/in³GB/1033
Water Absorption 0.60 %0.60 %23°C•24h
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 60.0 MPa8700 psiGB/1040
Elongation at Break 2.0 %2.0 %GB/1040
Flexural Strength 100 MPa14500 psiGB/9341
Flexural Modulus 8.80 GPa1280 ksiGB/9341
Charpy Impact Unnotched 2.00 J/cm²9.52 ft-lb/in²IS0179-1:2000
Charpy Impact, Notched 0.500 J/cm²2.38 ft-lb/in²IS0179-1:2000
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmGB/1410
Comparative Tracking Index 550 V550 VGB/4207
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 150 °C302 °FGB1634
Flammability, UL94 V-0V-0GB/T2408
 
Processing PropertiesMetricEnglishComments
Processing Temperature 225 - 250 °C437 - 482 °F
Mold Temperature 60.0 - 90.0 °C140 - 194 °F
Drying Temperature  110 °C
@Time 18000 sec
230 °F
@Time 5.00 hour
Chute Hot-Wind
 110 °C
@Time 18000 sec
230 °F
@Time 5.00 hour
Horizontal Oven
 110 °C
@Time 7200 sec
230 °F
@Time 2.00 hour
Vacuum Pressure, -0.08 MPa
Injection Pressure 80.0 - 100 MPa11600 - 14500 psi
 
Descriptive Properties
Speed of Shoot, %35-80

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese SO.F.TER Nylfor B® B2 FR2/3A Polyamide 6
Zhejiang Juner PA-A5 Flame-Retardant & Mineral Reinforced PA6
Zhejiang Juner PA-A4 Flame-Retardant & Mineral Reinforced PA6
Röhm ACRYLITE® Soundstop BirdGuard, Acrylic
INEOS Styrolution Luran® S KR2858 G3 Acrylonitrile Styrene Acrylate (ASA)

PJUNER52 / 48565

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.