MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

A. Schulman LP552-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Impact Grade

Material Notes: Description

LP 552-01 is a U.L. approved narrow molecular weight copolymer high-density polyethylene combining good flow with excellent stiffness and cold temperature impact strength. It has good toughness and stress crack resistance.
Application

Applications of LP 552-01 include food storage containers, housewares, toys, overcaps, and closures. This resin meets FDA Regulation CFR 177.1520 (c) 3.1.
Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.953 g/cc0.953 g/ccASTM D792
ESCR 100% Igepal® 1.0 hour1.0 hourCondition B; ASTM D1693
Melt Index of Compound 20 g/10 min20 g/10 minCondition E; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 22.1 MPa3200 psiASTM D638
Elongation at Break 100 %100 %ASTM D638
Flexural Modulus, 1% Secant 827 MPa120000 psiASTM D790
Falling Dart Impact 176 J
@Temperature -40.0 °C
130 ft-lb
@Temperature -40.0 °F
F50; ASTM D3056
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman LP552-01 Injection Molding, Extrusion Grade Compound
Network Polymers NPP 50-0151
A. Schulman LP551-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene
Network Polymers NPP 50-0350
Network Polymers NPP 50-0863

PASHU086 / 25050

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.