MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Dow DOWLEX™ IP-42 High Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Impact Grade

Material Notes: DOWLEX® IP-42 resin is an improved processing high density polyethylene resin designed for excellent flow and high impact. DOWLEX IP-42 resin is designed by optimizing the breadth and shape of the molecular weight distribution and peak molecular weight with a slightly lower density for increased impact strength. Typical applications are housewares, ice cream and promo applications. This material complies with FDA regulation 21 CFR 177.1520 (c) 3.1 for food contact applications. The regulation should be consulted for complete details.

Data provided by Dow Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.948 g/cc0.0342 lb/in³
Viscosity  47000 cP
@Shear Rate 5000 1/s,
Temperature 190 °C
47000 cP
@Shear Rate 5000 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
 87000 cP
@Shear Rate 1000 1/s,
Temperature 190 °C
87000 cP
@Shear Rate 1000 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
 132000 cP
@Shear Rate 300 1/s,
Temperature 190 °C
132000 cP
@Shear Rate 300 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
Melt Flow 42 g/10 min
@Load 2.16 kg
42 g/10 min
@Load 4.76 lb
Melt flow ratio I10/I2 is 8.5.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 10.0 MPa1450 psi
Tensile Strength, Yield 19.0 MPa2760 psi
Elongation at Break 300 %300 %
Modulus of Elasticity 0.565 GPa81.9 ksiMolded Sample 2% Secant Modulus
Flexural Modulus 0.834 GPa121 ksi
Izod Impact Resistance 2.90 J/cm²13.8 ft-lb/in²
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 118 °C244 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow HDPE 12450N High Density Polyethylene
Dow DMDA-8920 NT 7 High Density Polyethylene Resin
Dow DOWLEX™ IP-22 High Density Polyethylene
Dow DMDA-8007 NT 7 High Density Polyethylene Resin
Dow DMDA-8904 NT 7 High Density Polyethylene Resin

PDW463 / 34532

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.