MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

NOVA Chemicals Sclair® 94E Butene LMDPE Film and Extrusion Resin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Medium Density (MDPE); Linear Medium Density Polyethylene (LMDPE), Film

Material Notes:

Features:

  • Excellent processability
  • Good stiffness and strength
  • High stretchability
  • Applications:

  • Overwrap film
  • Netting
  • Blend resin
  • Information provided by Nova Chemicals

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 0.936 g/cc0.0338 lb/in³ASTM D792
    Thickness 25.0 microns0.984 mil
    Melt Flow 1.8 g/10 min
    @Load 2.16 kg,
    Temperature 190 °C
    1.8 g/10 min
    @Load 4.76 lb,
    Temperature 374 °F
    ASTM D1238
     
    Mechanical PropertiesMetricEnglishComments
    Hardness, Shore D 6060ASTM D2240
    Tensile Strength at Break 30.0 MPa4350 psiASTM D638
    Tensile Strength, Yield 17.2 MPa2500 psiASTM D638
    Elongation at Break 1100 %1100 %ASTM D638
    Puncture Energy 0.275 J0.203 ft-lbLow Friction Puncture
    Elmendorf Tear Strength MD 19 g19 gASTM D1922
    Elmendorf Tear Strength TD 140 g140 gASTM D1922
    Dart Drop Test 40.0 g0.0882 lbASTM D1709/A
     
    Thermal PropertiesMetricEnglishComments
    Melting Point 124 °C255 °FNOVA
    Vicat Softening Point 119 °C246 °FASTM D1525
    Brittleness Temperature <= -75.0 °C<= -103 °FASTM D746

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    LyondellBasell Alathon® L5045 High Density Polyethylene
    Ineos T50-2000 HDPE
    Ineos J50-2000-119 HDPE
    Formosa Plastics Formolene® HL3812 Film (Hexene) HDPE
    Dow HDPE 38152M High Density Polyethylene

    PNOV922 / 54868

    Proto3000 – 3D Engineering Solutions

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.