MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

NOVA Chemicals Surpass® FPs021-F Octene sLLDPE Film Resin, 25 Micron Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Octene, Film

Material Notes: FPs021-F complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.

NOVA Chemicals' polyethylene resins are biologically and chemically inert.

Features: Good stiffness, Easy processability, Very good toughness and strength, Excellent seal properties, Low gel

Additives: Process stabilizer, Antiblock at 3400 ppm, Polymer process aid

Applications: Heavy duty shipping sacks requiring very good toughness and high stiffness, Industrial packaging, Industrial liners, Lamination film

Film properties are typical of blown film extruded on a 2.5" extruder with 4" die and 35-mil die gap at a blow up ratio of 2.5:1, but are dependent upon operating conditions.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.921 g/cc0.0333 lb/in³ASTM D 792
Thickness 25.0 microns0.984 milAs tested for properties on this data sheet
 25.0 - 150 microns0.984 - 5.91 milRecommended range for processing
Melt Flow 0.80 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.80 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 9.00 MPa1310 psiASTM D 882
Film Tensile Strength at Yield, TD 10.0 MPa1450 psiASTM D 882
Film Elongation at Break, MD 520 %520 %ASTM D 882
Film Elongation at Break, TD 700 %700 %ASTM D 882
Elmendorf Tear Strength MD 290 g290 gASTM D 1922
Elmendorf Tear Strength TD 490 g490 gASTM D 1922
Elmendorf Tear Strength, MD 11.6 g/micron295 g/milASTM D 1922
Elmendorf Tear Strength, TD 19.6 g/micron498 g/milASTM D 1922
Dart Drop 20.5 g/micron521 g/milASTM D 1709/A
Dart Drop Test 512 g1.13 lbF50; ASTM D 1709/A
Film Tensile Strength at Break, MD 50.0 MPa7250 psiASTM D 882
Film Tensile Strength at Break, TD 42.0 MPa6090 psiASTM D 882
1% Secant Modulus, MD 174 MPa25200 psiASTM D 882
1% Secant Modulus, TD 188 MPa27300 psiASTM D 882
 
Optical PropertiesMetricEnglishComments
Haze 21 %21 %ASTM D 1003
Gloss 33 %33 %At 45°; ASTM D 2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 200 - 230 °C392 - 446 °FRecommended
Die Opening 0.0889 - 0.203 cm0.0350 - 0.0800 inRecommended range
 
Descriptive Properties
Low Friction Puncture53 (J/mm)NOVA Chemicals test method

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NOVA Chemicals Surpass® FPs117-C Octene Copolymer sLLDPE Film Resins
NOVA Chemicals Surpass® FPs021-F Octene sLLDPE Film Resin, 75 Micron Film
NOVA Chemicals Surpass® FPs016-C Octene sLLDPE Film Resin
NOVA Chemicals Surpass® FPs225-A Octene Copolymer sLLDPE Film Resin
NOVA Chemicals Sclair® FP019-D Octene Copolymer LLDPE Film Resin

PNOV771 / 108896

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.