Covestro Baygal® 90 IK 51 Polyurethane
(discontinued **)
Categories:
Polymer
;
Thermoset
;
Polyurethane, TS
;
Thermoset Polyurethane, Liquid, Quartz Filled
Material Notes:
Uses: Suitable for the solid insulation of measuring transducers.
Information provided by Bayer.
As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.76
g/cc
0.0636
lb/in³
Water Absorption at Saturation
0.060 %
0.060 %
0.060 %
0.060 %
Mechanical Properties
Metric
English
Comments
Tensile Strength, Ultimate
84.0
MPa
12200
psi
Elongation at Break
1.4 %
1.4 %
Tensile Modulus
9.00
GPa
1310
ksi
Electrical Properties
Metric
English
Comments
Electrical Resistivity
>=
1.00e+15
ohm-cm
>=
1.00e+15
ohm-cm
Surface Resistance
>=
1.00e+15
ohm
>=
1.00e+15
ohm
Dielectric Constant
4.0
@Frequency 1e+6 Hz
4.0
@Frequency 1e+6 Hz
4.3
@Frequency 100 Hz
4.3
@Frequency 100 Hz
Dielectric Strength
29.0
kV/mm
737
kV/in
Dissipation Factor
0.011
@Frequency 1e+6 Hz
0.011
@Frequency 1e+6 Hz
0.013
@Frequency 100 Hz
0.013
@Frequency 100 Hz
Comparative Tracking Index
600
V
600
V
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
40.0
µm/m-°C
@Temperature 20.0 °C
22.2
µin/in-°F
@Temperature 68.0 °F
CTE, linear, Transverse to Flow
40.0
µm/m-°C
@Temperature 20.0 °C
22.2
µin/in-°F
@Temperature 68.0 °F
Glass Transition Temp, Tg
90.0
°C
194
°F
Oxygen Index
29 %
29 %
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Covestro Acclaim® 8200 Polyol
Covestro Baygal® 90 IK 20 Polyurethane
BCC Products Proto-Kast BC 8163 Urethane Casting
BCC Products DP-11-90 Urethane Casting
BCC Products BC 8870 Polyurethane Elastomer
PBA071 / 26683
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.