MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Desktop Metal Ti64 Studio System™ 3D Printed; As-Sintered
Categories: Metal; 3D Printing/Additive Manufacturing Metal; Nonferrous Metal; Titanium Alloy; Alpha/Beta Titanium Alloy

Material Notes: Ti64 is ideal for prototyping medical devices such as tweezers, forceps, clamps, suture instruments as well as for 3D printing specialty automotive components, including connecting rods and gearboxes for racing. Its material properties are well known to be a high strength-to-weight ratio and corrosion resistance.

Applications:

  • Automotive
  • Consumer Goods
  • Connecting Rods
  • Sporting Goods
  • Medical Devices
  • Jewelry

Information provided by Proto3000

Key Words: Bound Metal Deposition Binder Jetting, UNS R56400
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.32 g/cc0.156 lb/in³
Porosity 2.5 %2.5 %ASTM B311
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 845 MPa123000 psiASTM E8M
Tensile Stress  200 MPa
@Strain 0.1 %
29000 psi
@Strain 0.1 %
 600 MPa
@Strain 0.3 %
87000 psi
@Strain 0.3 %
 825 MPa
@Strain 1.5 %
120000 psi
@Strain 1.5 %
Tensile Strength, Yield 730 MPa106000 psiASTM E8M
Elongation at Break 17.0 %17.0 %ASTM E8M
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 5.50 - 6.75 %5.50 - 6.75 %
Titanium, Ti 88.75 - 91.0 %88.75 - 91.0 %Balance
Vanadium, V 3.50 - 4.50 %3.50 - 4.50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NPROTO891 / 322904

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.